会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 3. 发明申请
    • INDUCTOR
    • 电感器
    • US20080303624A1
    • 2008-12-11
    • US12133614
    • 2008-06-05
    • Seiichi YAMADAOkikuni TakahataHiroyuki KamataFumishirou TsudaMasahiro Kondo
    • Seiichi YAMADAOkikuni TakahataHiroyuki KamataFumishirou TsudaMasahiro Kondo
    • H01F27/24
    • H01F17/043H01F3/14H01F27/2847
    • An inductor includes a first magnetic substance core which has a middle leg, a first outer leg, a second outer leg, and a body portion interconnecting the middle leg, the first outer leg and the second outer leg, and a second magnetic substance core which is arranged to be opposed to the first magnetic substance core. A first conductor is arranged in a first space which is formed by the middle leg, the first outer leg, part of the body portion, and the second magnetic substance core. A second conductor is arranged in a second space which is formed by the middle leg, the second outer leg, part of the body portion, and the second magnetic substance core. The middle leg is formed with a region which is lower in height than the first outer leg, in the same direction as the longitudinal direction of the first outer leg.
    • 电感器包括第一磁性体芯,其具有中间腿,第一外腿,第二外腿和互连中腿,第一外腿和第二外腿的主体部,以及第二磁性体芯, 被布置成与第一磁性体芯相对。 第一导体布置在由中间腿,第一外腿,主体部分和第二磁性体芯构成的第一空间中。 第二导体布置在由中腿,第二外腿,主体部分和第二磁性体芯构成的第二空间中。 中间腿在与第一外腿的长度方向相同的方向上形成有比第一外腿低的区域。
    • 6. 发明授权
    • Alumina substrate and method of manufacturing same
    • 氧化铝基板及其制造方法
    • US4045412A
    • 1977-08-30
    • US595703
    • 1975-07-14
    • Seiichi YamadaKyohei Murakawa
    • Seiichi YamadaKyohei Murakawa
    • B28B1/30C04B35/111H05K1/03C04B35/64C04B35/10
    • C04B35/111H05K1/0306
    • An improved alumina substrate comprising alumina and magnesium oxide has a surface finish of no more than 0.05 .mu.m CLA and a density of at least 3.90 g/cm.sup.3 in an as-fired condition and is composed of alumina grains which are sufficiently grown to have straight grain boundaries and flat surfaces to form a surface of the substrate. The improved substrate is produced by firing a green sheet having a high content of raw material powder and a density of more than 2.60 g/cm.sup.3 at a temperature of 1525.degree. to 1650.degree. C. The green sheet with high density is formed by the process of aggregating an organic agent and a high purity alumina powder by dry milling and casting the resultant slip.
    • 包含氧化铝和氧化镁的改进的氧化铝基材在烧制条件下具有不超过0.05μm的CLA的表面光洁度和至少3.90g / cm 3的密度,并且由氧化铝颗粒组成,其被充分生长以具有直 晶界和平坦表面以形成基底的表面。 通过在1525℃〜1650℃的温度下焙烧原料粉末含量高,密度大于2.60g / cm 3的生片,制造改良的基材。通过该方法形成高密度的生片 通过干磨和铸造所得到的滑移来聚集有机试剂和高纯度氧化铝粉末。