    • 1. 发明授权
    • Method of inhibiting cold-rolled steel sheet edge cracking, and method of producing the steel sheet
    • 冷轧钢板边缘裂纹的抑制方法,钢板的制造方法
    • US06749701B2
    • 2004-06-15
    • US10287634
    • 2002-11-05
    • Naoto HiramatsuKouki TomimuraSeiichi Isozaki
    • Naoto HiramatsuKouki TomimuraSeiichi Isozaki
    • C21D8007
    • C21D6/004C21D8/0205C21D8/0436C21D8/0468C21D2211/008C22C38/001C22C38/54
    • A high-strength, high-toughness martensitic stainless steel sheet has a chemical composition comprising, in mass percent, more than 0.03 to 0.15% of C, 0.2-2.0% of Si, not more than 1.0% of Mn, not more than 0.06% of P, not more than 0.006% of S, 2.0-5.0% of Ni, 14.0-17.0% of Cr, more than 0.03 to 0.10% of N, 0.0010-0.0070% of B, and the balance of Fe and unavoidable impurities and has an A value of not less than −1.8, where A value=30(C+N)−1.5Si+0.5Mn+Ni−1.3Cr+11.8. The suitability of the steel sheet as a gasket material is enhanced by producing it to include not less than 85 vol % of martensite phase and to have a spring bending elastic limit Kb0.1 after application of tensile strain of 0.1% of not less than 700 N/mm2. Edge cracking during cold rolling is inhibited by conducting cold rolling after subjecting the hot-rolled sheet to 600-800° C.×10 hr or less intermediate annealing to impart a steel hardness of not greater than Hv 380.
    • 高强度,高韧性的马氏体系不锈钢板的化学成分以质量%计含有C:0.03〜0.15%,Si:0.2〜2.0%,Mn:1.0%以下,0.06以下 P的%以下,S:0.006%以下,Ni:2.0〜5.0%,Cr:14.0〜17.0%,N:0.03〜0.10%,B:0.0010〜0.0070%,Fe:不可避免的杂质 并且具有不小于-1.8的A值,其中A值= 30(C + N)-1.5Si + 0.5Mn + Ni-1.3Cr + 11.8。 钢板作为垫片材料的适用性通过将其制成包括不小于85体积%的马氏体相并且在施加不小于700的0.1%的拉伸应变之后具有弹性弯曲弹性极限Kb0.1来增强 N / mm 2。 在将热轧板进行600-800℃×10小时以上的中间退火后,进行冷轧,赋予不高于Hv380的钢硬度,可以抑制冷轧时的边缘裂纹。
    • 3. 发明授权
    • High-strength, high-toughness martensitic stainless steel sheet
    • 高强度,高韧性马氏体不锈钢板
    • US06488786B2
    • 2002-12-03
    • US09759349
    • 2001-01-16
    • Naoto HiramatsuKouki TomimuraSeiichi Isozaki
    • Naoto HiramatsuKouki TomimuraSeiichi Isozaki
    • C22C3832
    • C21D6/004C21D8/0205C21D8/0436C21D8/0468C21D2211/008C22C38/001C22C38/54
    • A high-strength, high-toughness martensitic stainless steel sheet has a chemical composition comprising, in mass percent, more than 0.03 to 0.15% of C, 0.2-2.0% of Si, not more than 1.0% of Mn, not more than 0.06% of P, not more than 0.006% of S, 2.0-5.0% of Ni, 14.0-17.0% of Cr, more than 0.03 to 0.10% of N, 0.0010-0.0070% of B, and the balance of Fe and unavoidable impurities and has an A value of not less than −1.8, where A value=30(C+N)−1.5Si+0.5Mn+Ni−1.3Cr+11.8. The suitability of the steel sheet as a gasket material is enhanced by producing it to include not less than 85 vol % of martensite phase and to have a spring bending elastic limit Kb0.1 after application of tensile strain of 0.1% of not less than 700 N/mm2. Edge cracking during cold rolling is inhibited by conducting cold rolling after subjecting the hot-rolled sheet to 600-800 ° C.×10 hr or less intermediate annealing to impart a steel hardness of not greater than Hv 380.
    • 高强度,高韧性的马氏体系不锈钢板的化学成分以质量%计含有C:0.03〜0.15%,Si:0.2〜2.0%,Mn:1.0%以下,0.06以下 P的%以下,S:0.006%以下,Ni:2.0〜5.0%,Cr:14.0〜17.0%,N:0.03〜0.10%,B:0.0010〜0.0070%,Fe:不可避免的杂质 并且具有不小于-1.8的A值,其中A值= 30(C + N)-1.5Si + 0.5Mn + Ni-1.3Cr + 11.8。 钢板作为垫片材料的适用性通过将其制成包括不小于85体积%的马氏体相并且在施加不小于700的0.1%的拉伸应变之后具有弹性弯曲弹性极限Kb0.1来增强 N / mm2。 在将热轧板进行600-800℃×10小时以上的中间退火后,进行冷轧,赋予不高于Hv380的钢硬度,可以抑制冷轧时的边缘裂纹。