    • 2. 发明申请
    • WELDING METHOD USING LASER BEAM
    • 使用激光束的焊接方法
    • WO1983002414A1
    • 1983-07-21
    • PCT/JP1983000004
    • 1983-01-07
    • KAWASAKI STEEL CORPORATIONSASAKI, HiroakiNISHIYAMA, NoboruKAMADA, Akio
    • KAWASAKI STEEL CORPORATION
    • B23K26/00
    • B23K26/147B23K1/0056B23K26/18B23K26/211B23K26/24B23K2103/04B23K2103/05
    • PCT No. PCT/JP83/00004 Sec. 371 Date Sep. 8, 1983 Sec. 102(e) Date Sep. 8, 1983 PCT Filed Jan. 7, 1983 PCT Pub. No. WO83/02414 PCT Pub. Date Jul. 21, 1983.A welding process using a laser beam for joining metals such as steel plates along a see-through groove 10 such as a square groove formed by laser welding between opposed edges of the two metals is disclosed, in which a filler wire 9 is supplied to the see-through groove 10 as shown in FIGS. 3a, 3b and 4 to increase the permissible gap of the see-through groove. A spot 11 of laser beam 1 with a power density of 5x105 w/cm2 or above is formed in the see-through groove 10 on the same level as the surface of the metals 3. The filler wire 9 is inserted into a point coincident with the spot 11 of the laser beam 1, or the spot 11 of the laser beam 1 is formed on top of the filler wire 9 in the see-through groove 10. As the filler wire 9 is melted by the laser beam, a globule or droplet formed is formed from it and proceeds to and deposited on the opposed edge faces 12 defining the groove 10 to heat the edges 12 to effect welding.
    • PCT No.PCT / JP83 / 00004 Sec。 371日期1983年9月8日 102(e)日期1983年9月8日PCT提交1983年1月7日PCT公布。 第WO83 / 02414号公报 日期:1983年7月21日。公开了一种使用激光束将金属(诸如钢板)沿着诸如通过两个金属的相对边缘之间的激光焊接形成的方形沟槽的透视槽10接合的焊接工艺,其中 填充线9被供应到透视槽10,如图1和2所示。 3a,3b和4以增加透明槽的允许间隙。 激光束1的功率密度为5×10 5 W / cm 2以上的点11在与金属3的表面相同的高度的贯通槽10上形成。填充线9插入与 激光束1的点11或激光束1的光斑11形成在透明槽10中的填充焊丝9的顶部上。当焊丝9被激光束熔化时, 形成的液滴由其形成并进行并沉积在限定槽10的相对的边缘面12上,以加热边缘12以实现焊接。