    • 1. 发明授权
    • Method for recovering metals from waste aluminum catalyst
    • 从废铝催化剂中回收金属的方法
    • US08986634B2
    • 2015-03-24
    • US13889070
    • 2013-05-07
    • Ping-Tao Wu
    • Ping-Tao Wu
    • C22B4/00C22B3/00C22B21/00
    • C22B23/0446C22B21/003Y02P10/234
    • The present invention refers to a method being easy to recover metals including nickel and aluminum from waste aluminum catalysts, thereby entirely promoting the recovering rate. Said method comprises: preparing and roasting a waste aluminum catalyst with sodium salts, and then obtaining a first solution comprising vanadium and molybdenum, and a dreg comprising nickel and aluminum through leaching and filtrating; collecting and mixing the dreg with alkali powders to obtain a mixture of the dreg and alkali powders, roasting the mixture at 300 to 1000° C. with aluminum in the dreg reacting with hydroxyl generated from the roasting of mixture and further generating aluminum hydroxide, and then obtaining a second solution comprising aluminum and a concentrate having nickel through another leaching and filtrating; and recovering aluminum from the second solution and recovering nickel from the concentrate.
    • 本发明涉及易于从废铝催化剂中回收包括镍和铝的金属的方法,从而完全提高回收率。 所述方法包括:用钠盐制备和焙烧废铝催化剂,然后通过浸出和过滤获得包含钒和钼的第一溶液和包含镍和铝的渣, 用碱粉末收集和混合该渣,得到该渣和碱粉末的混合物,在该混合物中,与该混合物焙烧产生的羟基反应,在300-1000℃下用铝烧结该混合物并进一步产生氢氧化铝,以及 然后通过另一次浸出和过滤获得包含铝和具有镍的浓缩物的第二溶液; 并从第二溶液中回收铝并从浓缩物中回收镍。
    • 2. 发明申请
    • METHOD FOR RECOVERING METALS FROM WASTE ALUMINUM CATALYST
    • 从废物铝催化剂中回收金属的方法
    • US20140286840A1
    • 2014-09-25
    • US13889070
    • 2013-05-07
    • Ping-Tao WU
    • Ping-Tao WU
    • C22B3/00C22B21/00
    • C22B23/0446C22B21/003Y02P10/234
    • The present invention refers to a method being easy to recover metals including nickel and aluminum from waste aluminum catalysts, thereby entirely promoting the recovering rate. Said method comprises: preparing and roasting a waste aluminum catalyst with sodium salts, and then obtaining a first solution comprising vanadium and molybdenum, and a dreg comprising nickel and aluminum through leaching and filtrating; collecting and mixing the dreg with alkali powders to obtain a mixture of the dreg and alkali powders, roasting the mixture at 300 to 1000° C. with aluminum in the dreg reacting with hydroxyl generated from the roasting of mixture and further generating aluminum hydroxide, and then obtaining a second solution comprising aluminum and a concentrate having nickel through another leaching and filtrating; and recovering aluminum from the second solution and recovering nickel from the concentrate.
    • 本发明涉及易于从废铝催化剂中回收包括镍和铝的金属的方法,从而完全提高回收率。 所述方法包括:用钠盐制备和焙烧废铝催化剂,然后通过浸出和过滤获得包含钒和钼的第一溶液和包含镍和铝的渣, 用碱粉末收集和混合该渣,得到该渣和碱粉末的混合物,在该混合物中,与该混合物焙烧产生的羟基反应,在300-1000℃下用铝烧结该混合物并进一步产生氢氧化铝,以及 然后通过另一次浸出和过滤获得包含铝和具有镍的浓缩物的第二溶液; 并从第二溶液中回收铝并从浓缩物中回收镍。