    • 3. 发明申请
    • HIGH-DENSITY POLYETHYLENE COMPOSITIONS, METHOD OF MAKING THE SAME, WIRE AND CABLE JACKETS MADE THEREFROM, AND METHOD OF MAKING SUCH WIRE AND CABLE JACKETS
    • WO2007130553A3
    • 2007-11-15
    • PCT/US2007/010796
    • 2007-05-02
    • DOW GLOBAL TECHNOLOGIES INC.KMIEC, Chester, J.MICHIE, William, J. Jr.,
    • KMIEC, Chester, J.MICHIE, William, J. Jr.,
    • C08L23/04H01B3/44
    • The instant invention is a high-density polyethylene composition, method of producing the same, wire and cable jackets made therefrom, and method of making such wire and cable jackets. The high-density polyethylene composition of the instant invention includes a first component, and a second component. The first component is a high molecular weight ethylene alpha-olefin copolymer having a density in the range of 0.915 to 0.940 g/cm 3 , and a melt index (I 21.6 ) in the range of 0.5 to 10 g/10 minutes. The second component is a low molecular weight ethylene polymer having a density in the range of 0.965 to 0.980 g/cm 3 , and a melt index (I 2 ) in the range of 50 to 1500 g/10 minutes. The high-density polyethylene composition has a melt index (I 2 ) of at least 1, a density in the range of 0.950 to 0.960 g/cm 3 , and g' of equal or greater than 1. The method of producing a high-density polyethylene composition includes the following steps: (1) introducing ethylene, and one or more alpha-olefin comonomers into a first reactor; (2) (co)polymerizing the ethylene in the presence of one or more alpha-olefin comonomers in the first reactor thereby producing a first component, wherein the first component being a high molecular weight ethylene alpha-olefin copolymer having a density in the range of 0.915 to 0.940 g/cm 3 , and a melt index (I 21.6 ) in the range of 0.5 to 10 g/10 minutes; (3) introducing the first component and additional ethylene into a second reactor; (4) polymerizing the additional ethylene in the second reactor thereby producing a second component, wherein the second component being a low molecular weight ethylene polymer having a density in the range of 0.965 to 0.980 g/cm 3 , and a melt index (I 2 ) in the range of 50 to 1500 g/10 minutes; and (5) thereby producing the high-density polyethylene composition, wherein the high-density polyethylene composition having a melt index (I 2 ) of at least 1, a density in the range of 0.950 to 0.960 g/cm 3 , and g' of equal or greater than 1. The wire and cable jackets according to instant invention comprise the above-described inventive high-density polyethylene composition, and such wire and cable jackets may be made via extrusion.