    • 7. 发明授权
    • Thermoplastic elastomer polyolefin in-reactor blends and molded articles therefrom
    • 热塑性弹性体聚烯烃反应器内共混物及其模塑制品
    • US08101685B2
    • 2012-01-24
    • US12638916
    • 2009-12-15
    • Peijun JiangArmenag H. DekmezianKevin R. SquireCesar A. Garcia-Franco
    • Peijun JiangArmenag H. DekmezianKevin R. SquireCesar A. Garcia-Franco
    • C08F8/00C08L23/04C08L23/10
    • C08L23/06C08L23/08C08L2205/02C08L2314/06C08L2666/06
    • This invention relates to an in-reactor polymer blend comprising: (a) a first ethylene-containing polymer having a density of greater than 0.90 g/cm3 and a Mw of more than 20,000 g/mol and (b) a second ethylene-containing polymer having a density of less than 0.90 g/cm3, wherein the polymer blend has a Tm of at least 90° C. (DSC second melt), a density of less than 0.92 g/cm3, and the densities of the first and second polymers differ by at least 1%. Specifically this invention relates to an in-reactor polymer blend comprising: (a) a first ethylene polymer comprising 90 to 100 wt % ethylene and from 0 to less than 10 wt % comonomer, said first ethylene polymer component having density of greater than 0.920 g/cm3, an Mw of 20,000 g/mol or more; and (b) a second ethylene polymer comprising from 70 to 90 wt % ethylene and 30 to 10 wt % comonomer, said second ethylene polymer having a density of 0.910 g/cm3 or less, wherein the polymer blend has: (a) a Tm of at least 100° C. over a density ranging from 0.84 to 0.92 g/cm3; (b) a elongation at break of 300% or more; (c) a strain hardening index M300/M100 of at least 1.2; (d) a ratio of complex viscosity at 0.01 rad/s to the viscosity at 100 rad/s is of at least 30; and (e) a shear thinning slope of the plot of log(dynamic viscosity) versus log(frequency) less than −0.2.
    • 本发明涉及一种反应器内聚合物共混物,其包含:(a)密度大于0.90g / cm 3,Mw大于20,000g / mol的第一含乙烯聚合物和(b)第二含乙烯的聚合物 聚合物的密度小于0.90g / cm 3,其中聚合物共混物具有至少90℃的Tm(DSC第二熔体),密度小于0.92g / cm 3,第一和第二密度 聚合物的差异至少为1%。 具体而言,本发明涉及一种反应器内聚合物共混物,其包含:(a)包含90至100重量%乙烯和0至小于10重量%共聚单体的第一乙烯聚合物,所述第一乙烯聚合物组分的密度大于0.920g / cm3,Mw为20,000g / mol以上; 和(b)包含70-90wt%乙烯和30-10wt%共聚单体的第二乙烯聚合物,所述第二乙烯聚合物的密度为0.910g / cm 3或更低,其中所述聚合物共混物具有:(a)Tm 至少100℃,密度范围为0.84至0.92g / cm 3; (b)断裂伸长率在300%以上; (c)至少为1.2的应变硬化指数M300 / M100; (d)0.01rad / s下的复数粘度与100rad / s下的粘度之比至少为30; 和(e)对数(动态粘度)对log(频率)小于-0.2的曲线的剪切变薄斜率。