    • 1. 发明专利
    • Method for manufacturing colored concrete kneaded material
    • 制造有色混凝土材料的方法
    • JP2003039422A
    • 2003-02-13
    • JP2001231658
    • 2001-07-31
    • Joetsu Shokai:KkTaiheiyo Cement Corp太平洋セメント株式会社株式会社 上越商会
    • OBATA AKIRAKAJIO SATOSHIICHIKAWA KATSUTOSHISATO TATSUZOHAO YUKIO
    • B28C7/12B28C5/42
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing a colored concrete kneaded material capable of preventing a residue (including a pigment) of the colored concrete kneaded material from being mixed within a normal concrete kneaded material in the case of manufacturing the colored concrete kneaded material and then the normal concrete kneaded material by using the same mixer.
      SOLUTION: The method for manufacturing the colored concrete kneaded material comprises a step of manufacturing the concrete kneaded material by removing a water quantity used in a slurry in the case of kneading concrete materials prepared according to a formula by a mixer, a step of preparing the slurry containing the pigment (100 pts.wt.), a water reducing agent (0.5 to 5.0 pts.wt. (in terms of a solid content)) and the water quantity (50 to 200 pts.wt.) and having a water flowing time of 10 s or less when measured by using a J
      14 funnel and a step of agitating the concrete kneaded material and the slurry by using an agitator (for example; an agitator carried at a concrete agitator truck).
      COPYRIGHT: (C)2003,JPO
    • 要解决的问题:提供一种制造着色混凝土搅拌材料的方法,该方法能够防止着色混凝土搅拌材料的残留物(包括颜料)在正常的混凝土搅拌材料中混合,在制造着色混凝土的情况下 材料,然后通过使用相同的搅拌机将普通混凝土搅拌材料。 解决方案:用于制造着色混凝土搅拌材料的方法包括如下步骤:在通过混合机捏合根据配方制备的混凝土材料的情况下,通过除去浆料中使用的水量来制造混凝土捏合材料;制备 含有颜料(100重量份),减水剂(0.5至5.0重量份(以固体含量计))和水量(50至200重量份)并具有水的浆料 通过使用J14漏斗测量10秒以下的流动时间,以及通过使用搅拌器(例如,在混凝土搅拌车上携带的搅拌器)搅拌混凝土搅拌物和浆料的步骤。