    • 2. 发明授权
    • Method of manufacturing retro-reflectives with excellent durability and wet retroreflectivity, and retro-reflectives manufactured thereby
    • 制造具有优异耐久性和抗回潮性的回流反射镜的方法,以及制造的反折射
    • KR100973980B1
    • 2010-08-05
    • KR20100009432
    • 2010-02-02
    • JEONG YOUNG HO
    • JEONG YOUNG HO
    • G02B5/128
    • G02B5/128B82Y30/00C03C12/02E01C23/166
    • PURPOSE: A method for manufacturing a retro-reflector and the retro-reflector are provided to improve embedding property with respect to the paint of a traffic lane by including titanium dioxide as a light reflector. CONSTITUTION: A thermosetting reflective adhesive layer(2), which is non-reactive at the room-temperature, is formed on the surface of core-glass-beads(1) and is composed of titanium dioxide as a light reflector and a thermosetting reflective resin composition which is non-reactive at the room-temperature. Glass-beads(3) are oriented onto the thermosetting reflective adhesive layer at a constant embedding rate. A hybrid coating layer(4) fills spaces between the oriented glass beads is composed of either of an organic-inorganic hybrid coating solution or a nano-sol-gel hybrid solution.
    • 目的:提供一种用于制造后向反射器和后向反射器的方法,以通过包括二氧化钛作为光反射器来改善相对于行车道的涂料的嵌入性能。 构成:在芯玻璃珠(1)的表面上形成在室温下不反应的热固性反射性粘合剂层(2),由二氧化钛作为光反射体和热固反射型 在室温下不反应的树脂组合物。 玻璃珠(3)以恒定的嵌入速率定向到热固性反射粘合剂层上。 混合涂层(4)填充由有机 - 无机杂化涂层溶液或纳米溶胶 - 凝胶混合溶液之一组成的定向玻璃珠之间的空间。
    • 7. 发明申请
    • METHOD FOR PRODUCING ARTIFICIAL LIGHTWEIGHT AGGREGATES USING COLD- OR HOT-ROLLED MILL SLUDGE
    • 使用冷轧或热轧工艺生产人造轻质聚合物的方法
    • WO2010101412A3
    • 2010-11-25
    • PCT/KR2010001329
    • 2010-03-03
    • CERAGREEN CO LTDJEONG YOUNG HO
    • JEONG YOUNG HO
    • C04B18/18C04B14/10
    • C04B18/027Y02W30/91Y02W30/94C04B14/10C04B18/023C04B18/0418C04B18/149
    • The present invention relates to a method for producing artificial lightweight aggregates using cold- or hot-rolled mill sludge and clay as a main material. More particularly, the present invention relates to a method for producing artificial lightweight aggregates, in which the aggregates are produced from cold- or hot-rolled mill sludge and clay as a primary material, and the aggregates have an absolute dry specific gravity of 0.8 to 1.5 and an absorptance of 5 to 20%. As the artificial lightweight aggregates according to the present invention use cold- or hot-rolled mill sludge, which is a by-product of the steel industry, as a main material, the necessity of an additional foaming agent is eliminated, and steel wastes are reutilized to increase economical advantages, reduce wastes, and prevent environmental contamination.
    • 本发明涉及使用冷轧或热轧轧机淤渣和粘土作为主要材料生产人造轻质集料的方法。 更具体地说,本发明涉及一种生产人造轻质集料的方法,其中集料由冷轧或热轧轧制污泥和作为主要材料的粘土制备,并且该集料的绝对干比重为0.8至 1.5和5至20%的吸收率。 由于根据本发明的人造轻质集料使用作为钢铁工业副产品的冷轧或热轧轧机污泥作为主要材料,因此消除了额外发泡剂的必要性,并且废钢是 重新利用以增加经济优势,减少废物,并防止环境污染。