    • 1. 发明授权
    • Process for suspension polymerization of vinyl chloride employing mixed
protective colloids
    • 使用混合保护胶体的氯乙烯的悬浮聚合方法
    • US4345056A
    • 1982-08-17
    • US959796
    • 1978-11-13
    • Helmut E. ThyretThomas BalweGerhard BeierJohann Bauer
    • Helmut E. ThyretThomas BalweGerhard BeierJohann Bauer
    • C08F14/00C08F2/00C08F2/18C08F2/20C08F14/06
    • C08F14/06
    • An improvement in the process of producing polyvinyl chloride by the suspension process in the presence of protective colloids by utilizing a protective colloid mixture of from 20% to 80% of the protective colloid mixture of a polyvinyl acetate having a hydrolysis degree of 40 to 55 mol % and the remainder of the protective colloid mixture of (1) a water-soluble polyvinyl alcohol having a hydrolysis degree of 70 to 90 mol %, or (2) an aminoethyl-hydroxypropyl cellulose having a molar substitution of from 0.05 to 1.5 mols of aminoethyl groups and 3 to 5 mols of hydroxypropyl groups, or (3) a vinyl acetate/vinyl pyrrolidone copolymer having a ratio of vinyl pyrrolidone to vinyl acetate in the copolymer of 50% to 70% by weight to 30% to 50% by weight and a K-value of 25 to 40. By the use of this protective colloid mixture, the polyvinyl chloride produced exhibits a large absorption of plasticizer and gives finished products having a low number of specks.
    • 通过使用水解度为40〜55mol的聚乙酸乙烯酯的保护胶体混合物的20〜80%的保护胶体混合物,在保护胶体存在下,通过悬浮法制备聚氯乙烯的方法的改进 %,其余的(1)水解度为70〜90摩尔%的水溶性聚乙烯醇的保护胶体混合物,或(2)摩尔取代度为0.05〜1.5摩尔的氨基乙基 - 羟丙基纤维素 氨基乙基和3至5摩尔羟丙基,或(3)共聚物中乙烯基吡咯烷酮与乙酸乙烯酯的比率为50重量%至70重量%至30重量%至50重量%的乙酸乙烯酯/乙烯基吡咯烷酮共聚物 并且K值为25〜40。通过使用该保护胶体混合物,所生产的聚氯乙烯显示出较大的增塑剂吸收,并产生具有少量斑点的成品。