    • METHOD OF UNIDIRECTIONAL SOLIDIFICATION OF CASTINGS AND ASSOCIATED APPARATUS
    • 铸造和相关设备的单向固化方法
    • WO2007009060A9
    • 2008-01-17
    • PCT/US2006027348
    • 2006-07-12
    • ALCOA INCCHU MEN GYU HOGIRON ALVAROKALLAHER KENNETH JSHAW JEFFREY J
    • CHU MEN GYU HOGIRON ALVAROKALLAHER KENNETH JSHAW JEFFREY J
    • B22D7/02B22D7/06
    • B22D7/02B22D7/06B22D7/064Y10S428/939Y10T428/12493Y10T428/12764
    • Molten metal is injected uniformly into a mold from a feed chamber in a horizontal or vertical direction at a controlled rate, directly on top of the metal already within the mold. A cooling medium is applied to the bottom surface of the substrate, with the type and flow rate of the cooling medium being varied to produce a controlled cooling rate throughout the casting process. The rate of introduction of molten metal and the flow rate of the cooling medium are both controlled to produce a relatively uniform solidification rate within the mold, thereby producing a uniform microstructure throughout the casting, and low stresses throughout the casting. A multiple layer ingot product is also provided comprising a base alloy layer and at least a first additional alloy layer, the two layers having different alloy compositions, where the first additional alloy layer is bonded directly to the base alloy layer by applying the first additional alloy in the molten state to the surface of the base alloy while the surface temperature of the base alloy is lower than the liquidus temperature and greater than eutectic temperature of the base alloy - 50 degrees Celsuis.
    • 熔融金属以受控的速率在水平或垂直方向上从进料室均匀地注入到模具中,直接在已经在模具内的金属的顶部上。 将冷却介质施加到基底的底表面,其中冷却介质的类型和流速被改变以在整个铸造过程中产生受控的冷却速率。 控制熔融金属的引入速率和冷却介质的流量都被控制以在模具内产生相对均匀的凝固速率,从而在铸件中产生均匀的微观结构,并且在整个铸件中产生低应力。 还提供了多层锭产品,其包括基底合金层和至少第一附加合金层,所述两层具有不同的合金组成,其中第一附加合金层通过施加第一附加合金直接结合到基底合金层 在基体合金的表面温度低于液相线温度并且大于基体合金的共晶温度(50℃Celsuis)时,处于熔融状态。
    • 2. 发明申请
    • METHOD OF UNIDIRECTIONAL SOLIDIFICATION OF CASTINGS AND ASSOCIATED APPARATUS
    • 单向凝固铸件及相关设备的方法
    • WO2007009060A3
    • 2007-10-25
    • PCT/US2006027348
    • 2006-07-12
    • ALCOA INCCHU MEN GYU HOGIRON ALVAROKALLAHER KENNETH JSHAW JEFFREY J
    • CHU MEN GYU HOGIRON ALVAROKALLAHER KENNETH JSHAW JEFFREY J
    • B22D7/02B22D7/06
    • B22D7/02B22D7/06B22D7/064Y10S428/939Y10T428/12493Y10T428/12764
    • Molten metal is injected uniformly into a mold from a feed chamber in a horizontal or vertical direction at a controlled rate, directly on top of the metal already within the mold. A cooling medium is applied to the bottom surface of the substrate, with the type and flow rate of the cooling medium being varied to produce a controlled cooling rate throughout the casting process. The rate of introduction of molten metal and the flow rate of the cooling medium are both controlled to produce a relatively uniform solidification rate within the mold, thereby producing a uniform microstructure throughout the casting, and low stresses throughout the casting. A multiple layer ingot product is also provided comprising a base alloy layer and at least a first additional alloy layer, the two layers having different alloy compositions, where the first additional alloy layer is bonded directly to the base alloy layer by applying the first additional alloy in the molten state to the surface of the base alloy while the surface temperature of the base alloy is lower than the liquidus temperature and greater than eutectic temperature of the base alloy - 50 degrees Celsuis.
    • 熔融金属从进料室以水平或垂直方向以受控速率均匀注入模具中,直接位于模具内已有金属的顶部。 将冷却介质施加到基底的底部表面,其中冷却介质的类型和流量变化以在整个浇铸过程中产生受控的冷却速率。 控制熔融金属的引入速率和冷却介质的流量以在模具内产生相对均匀的凝固速率,由此在整个铸造过程中产生均匀的微观结构,并且在整个铸造过程中具有低应力。 还提供了多层铸锭产品,其包括基础合金层和至少第一附加合金层,这两个层具有不同的合金成分,其中第一附加合金层通过将第一附加合金直接结合到基础合金层 在基体合金表面以熔融状态存在,而基体合金的表面温度低于液相温度并且大于基体合金的共晶温度-50摄氏度。
    • 3. 发明申请
    • METHOD OF UNIDIRECTIONAL SOLIDIFICATION OF CASTINGS AND ASSOCIATED APPARATUS
    • 铸造和相关设备的单向固化方法
    • WO2007009060A2
    • 2007-01-18
    • PCT/US2006/027348
    • 2006-07-12
    • ALCOA INC.CHU, Men, G.YU, HoGIRON, AlvaroKALLAHER, Kenneth, J.SHAW, Jeffrey, J.
    • CHU, Men, G.YU, HoGIRON, AlvaroKALLAHER, Kenneth, J.SHAW, Jeffrey, J.
    • B22D7/02B22D7/06
    • B22D7/02B22D7/06B22D7/064Y10S428/939Y10T428/12493Y10T428/12764
    • Molten metal is injected uniformly into a mold from a feed chamber in a horizontal or vertical direction at a controlled rate, directly on top of the metal already within the mold. A cooling medium is applied to the bottom surface of the substrate, with the type and flow rate of the cooling medium being varied to produce a controlled cooling rate throughout the casting process. The rate of introduction of molten metal and the flow rate of the cooling medium are both controlled to produce a relatively uniform solidification rate within the mold, thereby producing a uniform microstructure throughout the casting, and low stresses throughout the casting. A multiple layer ingot product is also provided comprising a base alloy layer and at least a first additional alloy layer, the two layers having different alloy compositions, where the first additional alloy layer is bonded directly to the base alloy layer by applying the first additional alloy in the molten state to the surface of the base alloy while the surface temperature of the base alloy is lower than the liquidus temperature and greater than eutectic temperature of the base alloy - 50 degrees Celsuis.
    • 熔融金属以受控的速率在水平或垂直方向上从进料室均匀地注入到模具中,直接在已经在模具内的金属的顶部上。 将冷却介质施加到基底的底表面,其中冷却介质的类型和流速被改变以在整个铸造过程中产生受控的冷却速率。 控制熔融金属的引入速率和冷却介质的流量都被控制以在模具内产生相对均匀的凝固速率,从而在铸件中产生均匀的微观结构,并且在整个铸件中产生低应力。 还提供了多层锭产品,其包括基底合金层和至少第一附加合金层,所述两层具有不同的合金组成,其中第一附加合金层通过施加第一附加合金直接结合到基底合金层 在基体合金的表面温度低于液相线温度并且大于基体合金的共晶温度(50℃Celsuis)时,处于熔融状态。