热词
    • 1. 发明授权
    • Length stabilized Nb-Sn wire and annealing method
    • 长度稳定的Nb-Sn丝和退火方法
    • US5104746A
    • 1992-04-14
    • US519700
    • 1990-05-04
    • Alan I. TaubMark L. Miller
    • Alan I. TaubMark L. Miller
    • H01L39/24
    • H01L39/2409Y10S428/93Y10T428/12486
    • A method for contraction annealing niobium-tin wire is disclosed. An improved niobium-tin wire is provided by loosely winding the wire on a mandrel, or by coiling the wire on a circumferentially retractile mandrel, and contraction annealing the wire without reaction-forming substantial amounts of Nb.sub.3 Sn. Such contraction annealing allows the wire to contract in length unconstrained thereby preventing the formation of internal tensile stresses in the wire and its surrounding insulation. Prevention of internal stresses in the wire greatly reduces the susceptibility of the wire to breakage, cracking, sintering, shorting, tin leakage, or substantial shifting of the wire from desired wrap positions when it is reaction annealed to form the brittle super-conducting intermetallic compound Nb.sub.3 Sn.
    • 公开了一种收缩退火铌锡丝的方法。 通过将线松散地缠绕在心轴上,或通过将线缠绕在周向可收缩的心轴上,并且在不反应形成大量Nb 3 Sn的情况下收缩退火线来提供改进的铌锡丝。 这种收缩退火允许电线长度收缩而不受约束,从而防止线材及其周围绝缘体内部拉伸应力的形成。 在进行反应退火处理时,预防线内部的应力会大大降低电线的断裂,开裂,烧结,短路,锡泄漏或电线从期望的缠绕位置实质上的偏移,从而形成脆性超导金属间化合物 Nb3Sn。
    • 7. 发明授权
    • Cold worked tri-nickel aluminide alloy compositions
    • 冷加工三镍铝合金组合物
    • US4676829A
    • 1987-06-30
    • US783723
    • 1985-10-03
    • Keh-Minn ChangAlan I. TaubShyh-Chin Huang
    • Keh-Minn ChangAlan I. TaubShyh-Chin Huang
    • C22C1/04C22C19/00C22C19/03C22C29/14
    • C22C19/007
    • Improvements in the positive temperature dependence of yield strength and in the work hardening rate of tri-nickel aluminide base alloys are achieved. The novel alloy composition has seven alloying ingredients as follows:______________________________________ ConcentrationIngredient in Atomic %______________________________________Ni balanceCo 8-12Al 16-20Si 4-6Nb 0.26-0.30Zr 0.02-0.04B 0.2-0.7______________________________________The novel composition may be prepared by forming a melt of the composition and atomizing the melt with an inert gas to form fine particles with Ll.sub.2 type crystal structure. The powder is densified by heat and pressure to a novel alloy composition having the improvements in positive temperature dependence of yield strength and work hardening rate as noted above.
    • 实现了三镍铝基合金的屈服强度和加工硬化率的正温度依赖性的改善。 新型合金成分具有以下七种合金成分: - 浓度 - 原子%-Ni平衡-Co 8-12 -Al 16-20 -Si 4-6 - Nb 0.26-0.30 -Zr 0.02-0.04 -B 0.2- 0.7 - 可以通过形成组合物的熔体并用惰性气体雾化熔体以形成具有Ll2型晶体结构的细颗粒来制备新组合物。 通过热和压力将粉末致密化成如上所述具有改善屈服强度和加工硬化率的正温度依赖性的新型合金组合物。