    • 86. 发明授权
    • Method of producing cold rolled steel sheets for deep drawing
    • 深冲压冷轧钢板的制造方法
    • US4576656A
    • 1986-03-18
    • US768927
    • 1985-08-26
    • Susumu SatohTakashi ObaraMinoru Nishida
    • Susumu SatohTakashi ObaraMinoru Nishida
    • C22C38/00C21D8/02C21D8/04C21D9/48C22C38/14
    • C21D8/0426C21D8/041
    • The present invention relates to a method of producing a cold rolled steel sheet for deep drawing. In order to improve the deep drawability (r-value), ductility (yield strength and elongation El) and the like of cold rolled sheet of ultra-low carbon aluminum killed steel, the chemical composition (% by weight) of the steel is adjusted such that the steel contains C: .ltoreq.0.015%, Mn: .ltoreq.0.4%, P: .ltoreq.0.03%, sol. Al: 0.005-0.100%, N: .ltoreq.0.010%, Ti (exclusive of Ti present in the form of oxide): in an amount satisfying a formula of ##EQU1## the hot rolling of the steel slab is effected at a soaking temperature lower than 1,100.degree. C. and at a finishing temperature of 600.degree.-780.degree. C. As illustrated in the drawings, a low temperature rolling can be carried out, and the resulting cold rolled steel sheet is excellent in the deep drawability and ductility and further excellent in the treatable property of the surface and in the surface property. Therefore, the cold rolled steel sheet is particularly suitable for the production of automotive exterior plate.
    • PCT No.PCT / JP83 / 00334 Sec。 371日期1984年3月15日 102(e)日期1984年3月15日PCT提交1983年10月7日PCT公布。 公开号WO84 / 01585 1984年4月26日。深拉深冷轧钢板的制造方法技术领域本发明涉及一种深拉深冷轧钢板的制造方法。 为了提高超低碳铝杀死钢的冷轧板的深冲性(r值),延展性(屈服强度和伸长率E1)等,调整钢的化学成分(重量%) 使得钢含有C:0.015%,Mn:0.4%,P:0.03%,溶胶。 Al:0.005-0.100%,N:<= 0.010%,Ti(以氧化物形式存在的Ti除外):满足公式“IMAGE”的钢的平均热轧是在均热 温度低于1100℃,最终温度为600〜-780℃。如图所示,可以进行低温轧制,所得到的冷轧钢板的深冲性和延展性优异 并且表面的可处理性能和表面性能也更优异。 因此,冷轧钢板特别适用于制造汽车外板。