会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 73. 发明授权
    • Device for mounting lamp on lamp mount
    • 用于将灯安装在灯座上的装置
    • US5186535A
    • 1993-02-16
    • US772842
    • 1991-10-08
    • Takashi Yokoyama
    • Takashi Yokoyama
    • F21S8/10F21V19/00
    • F21S48/1118
    • A device for mounting a lamp on a lamp mount includes an engagement spring made of a spring steel sheet in the form of a leaf spring having a substantially elliptical shape. The engagement spring is configured such that it extends at a right angle relative to the axis of a lamp socket, and moreover, it exhibits a line symmetry relative to two lines extending on a common plane at a right angle relative to each other. The common plane extends at a right angle relative to the axis of the lamp socket. The engagement spring includes an opposing pair of depressing portions and an opposing pair of arm-shaped engagement portions. The depressing portions extend in parallel with one of the two lines while maintaining a line symmetry relative to one of the two lines. The engagement portions are arranged in a spaced relationship while maintaining a line symmetry relative to other one of the two lines. When the engagement spring is placed in position on the upper surface of a lamp socket inserted through a socket insert hole, a uniform resilient depressing force is imparted to the lamp socket from the engagement spring so as to firmly hold the lamp socket on the lamp mount.
    • 用于将灯安装在灯座上的装置包括由具有大致椭圆形状的板簧形式的弹簧钢板制成的接合弹簧。 接合弹簧被构造成使得其相对于灯座的轴线成直角地延伸,并且此外,它相对于彼此相对于在公共平面上以直角延伸的两条线呈现线对称。 公共平面相对于灯座的轴线成直角延伸。 接合弹簧包括相对的一对按压部分和相对的一对臂形接合部分。 按压部分与两条线之一平行地延伸,同时保持相对于两条线之一的线对称。 接合部分以相互间隔的关系布置,同时保持相对于两条线中的另一条线的线对称。 当接合弹簧被放置在通过插座插入孔插入的灯插座的上表面上的适当位置时,从接合弹簧向灯插座施加均匀的弹性按压力,以将灯座牢固地保持在灯座上 。
    • 75. 发明授权
    • Soft magnetic stainless steel for cold forging
    • 软磁不锈钢用于冷锻
    • US4714502A
    • 1987-12-22
    • US886675
    • 1986-07-18
    • Yoshinobu HonkuraKouji MurataTakashi Yokoyama
    • Yoshinobu HonkuraKouji MurataTakashi Yokoyama
    • C22C38/00C22C38/28C22C38/60
    • C22C38/60
    • A soft magnetic stainless steel consists essentially of, by weight, up to 0.03% of C, 0.40 to 1.10% of Si, up to 0.50% of Mn, 9.0 to 19.0% of Cr, 0.31 to 0.60% of Al, 0.01 to 0.03% of S, 0.10 to 0.30% of Pb, 0.02 to 0.25% of Ti, 0.02 to 0.10% of Zr, and up to 0.03% of N, and the balance of Fe and inevitable impurities, with a proviso that the C+N content is not more than 0.04% and the Si+Al content is not more than 1.35%. The steel has a magnetic flux density of 13,000 G or more and a coercive force of 1.2 Oe or less as magnetic properties, and a tensile strength of 41 kgf/mm.sup.2 or less and a critical compressibility of 50% or more as formability in cold forging. The steel is suitable for manufacturing, by cold forging, parts with complex shapes such as cores of solenoid operated valves and electromagnetic clutches, and bodies of electronic fuel injection apparatuses for internal combustion engines.
    • 软磁性不锈钢主要由以下组成:C:0.03%以下,Si:0.40〜1.10%,Mn:0.50%以下,Cr:9.0〜19.0%,Al:0.01〜0.03, S的%,Pb的0.10〜0.30%,Ti的0.02〜0.25%,Zr的0.02〜0.10%以及N的0.03%以下,剩余的Fe和不可避免的杂质,条件是C + N 含量不大于0.04%,Si + Al含量不超过1.35%。 该钢的磁通密度为13000G以上,矫顽力为1.2Oe以下,磁性能,拉伸强度为41kgf / mm 2以下,临界压缩率为50%以上,作为冷锻成形性 。 该钢适用于通过冷锻制造具有复杂形状的部件,例如电磁阀和电磁离合器的核心,以及用于内燃机的电子燃料喷射装置的主体。
    • 80. 发明申请
    • LUMINESCENT PRODUCT AND PROCESS FOR PRODUCING THE SAME
    • 发光产品及其生产方法
    • US20090263665A1
    • 2009-10-22
    • US12375619
    • 2007-04-06
    • Takashi KamiikeTakashi Yokoyama
    • Takashi KamiikeTakashi Yokoyama
    • B32B27/40B28B1/20
    • B29C41/22B29C41/042B29K2995/0018B29L2031/7232Y10T428/31551
    • A luminescent product molded by centrifugal molding which is inhibited from curling and has a white layer for improving phosphorescent performance. The product comprises: a hiding layer formed from a first mixture which is a mixture of a first thermosetting resin and a pigment by subjecting the mixture to centrifugal molding with heating; a phosphorescent layer obtained from a second mixture which is a mixture of a second thermosetting resin and a phosphorescent pigment having a higher specific gravity than the second thermosetting resin by pouring the second mixture on the hiding layer and subjecting it to centrifugal molding with heating; and a transparent layer. The phosphorescent layer is located nearly at the center of the product thickness. Thus, the product can be effectively inhibited from curling.
    • 通过离心成型模制的发光产品被抑制卷曲,并具有白色层以提高磷光性能。 该产品包括:通过加热使混合物进行离心成型,由第一混合物形成的隐藏层,第一混合物是第一热固性树脂和颜料的混合物; 从第二混合物获得的磷光层,其是通过将第二混合物倾倒在隐藏层上并通过加热进行离心模塑而成为比例比第二热固性树脂高的第二热固性树脂和磷光颜料的混合物; 和透明层。 磷光层位于产品厚度的中心附近。 因此,可以有效地抑制产品的卷曲。