    • 61. 发明申请
    • POLYMER, POLYMER ELECTROLYTE AND USE OF SAME
    • 聚合物,聚合物电解质及其用途
    • US20110151355A1
    • 2011-06-23
    • US13059529
    • 2009-08-13
    • Arihiro YashiroShigeru Sasaki
    • Arihiro YashiroShigeru Sasaki
    • H01M8/10C08G75/20C08J5/22B01J31/06
    • C08G61/10C08J5/2256C08J2365/02C08J2371/12C08J2381/06H01B1/122H01M4/8668H01M8/1004H01M8/1023H01M8/1027H01M8/1032
    • The present invention provides a polymer, a polymer electrolyte and the use thereof. The polymer has, as a structural unit, a phenylene group in which two or three hydrogen atoms each have been substituted with a group represented by the following formula (A), and is insoluble in water: wherein A1 represents a group represented by formula (1a), formula (1b) or formula (1c) below, and the two or three A1 groups may be the same as or different from each other, wherein R10 and R11 each independently represents a hydrogen atom, an alkyl group of 1 to 20 carbon atoms, or an aryl group of 6 to 20 carbon atoms, R12 represents a hydrogen atom, an alkyl group of 1 to 20 carbon atoms, or an aryl group of 6 to 20 carbon atoms, M represents a metal ion or an ammonium ion, and in a case where M represents a divalent or higher-valent metal ion, M may be further bonded to another substituent.
    • 本发明提供聚合物,聚合物电解质及其用途。 聚合物作为结构单元具有其中两个或三个氢原子各自被下式(A)表示的基团取代的亚苯基,并且不溶于水:其中A1表示由式( 1a),式(1b)或式(1c),并且两个或三个A 1基团可以彼此相同或不同,其中R 10和R 11各自独立地表示氢原子,1〜20的烷基 碳原子或6〜20个碳原子的芳基,R 12表示氢原子,1〜20个碳原子的烷基或6〜20个碳原子的芳基,M表示金属离子或铵离子 ,并且在M表示二价或更高价金属离子的情况下,M可以进一步与另一取代基结合。
    • 65. 发明申请
    • THERMOPLASTIC COMPOSITION AND MOLDED ARTICLE THEREOF
    • 热塑性组合物及其制品
    • US20100105837A1
    • 2010-04-29
    • US12530640
    • 2008-03-25
    • Shigeru SasakiKatsunori Nitta
    • Shigeru SasakiKatsunori Nitta
    • C08L53/02C08L53/00
    • C08L53/025C08L23/02C08L23/10C08L23/12C08L25/06C08L53/02C08L71/12C08L2205/035C08L2666/02C08L2666/14C08L2666/04C08L2666/24
    • The present invention discloses a thermoplastic resin composition comprising: (A) 95 to 5 parts by weight of a styrenic resin and/or a polyphenylene ether resin; (B) 5 to 95 weight parts of an olefinic resin; and (C) 1 to 28 parts by weight of a partially hydrogenated block copolymer based on 100 parts by weight of the total amount of the components (A) and (B), wherein the component (C) comprises at least one polymer block X containing a vinyl aromatic compound as a main component and at least one polymer block Y containing a conjugated diene compound as a main component, a content of the vinyl aromatic compound in the component (C) is at least 10 wt % and at most 80 wt %, the vinyl bond content before hydrogenation in the component (C) is 3 wt % or more and less than 50 wt %, and 1 mol % or more and less than 40 mol % of double bonds derived from the conjugated diene compound in the block copolymer which constitutes the component (C) are hydrogenated.
    • 本发明公开了一种热塑性树脂组合物,其包含:(A)95〜5重量份的苯乙烯系树脂和/或聚苯醚树脂; (B)5〜95重量份的烯烃树脂; 和(C)基于100重量份的组分(A)和(B)的总量的1至28重量份的部分氢化嵌段共聚物,其中组分(C)包含至少一种聚合物嵌段X 含有乙烯基芳族化合物作为主要成分和至少一种含有共轭二烯化合物作为主要成分的聚合物嵌段Y,(C)成分中的乙烯基芳香族化合物的含量为10重量%以上80重量%以下 %,成分(C)中氢化前的乙烯基键含量为衍生自共轭二烯化合物的双键的3重量%以上且小于50重量%,1摩尔%以上且小于40摩尔% 构成组分(C)的嵌段共聚物被氢化。
    • 66. 发明申请
    • Method for Producing Polymer Compound
    • 生产高分子化合物的方法
    • US20100105786A1
    • 2010-04-29
    • US10588266
    • 2005-02-02
    • Toru OnoderaKazuel OhuchiShigeru Sasaki
    • Toru OnoderaKazuel OhuchiShigeru Sasaki
    • C08G16/00C08G75/00C08J5/20
    • H01M8/1023C08G61/00H01B1/122H01M8/0289H01M8/1067Y02P70/56
    • A method for polymerizing a monomer represented by the formula (1) or copolymerizing a monomer represented by the formula (1) and a monomer represented by the formula (2) in the co-presence of a condensation agent comprising a transition metal complex, to thereby produce a polymer compound represented by the formula (3): X1—Ar1—X2 (1) X3—Ar2—X4 (2) —(Ar1)q-(Ar2)r- (3) [X1, X2, X3 and X4 represent groups separating in the condensation, Ar1 represents a two-valent aromatic group having at least a sulfonic acid or a sulfonic acid via a connecting group as a substituent, q represents a positive number, r represents 0 or a positive number, and the sum of q and r is 300 or more], characterized in that the above condensation agent and the above monomer are mixed at a temperature of 45° C. or higher. The above method allows the production of a polymer compound which exhibits excellent fuel cell characteristics and has a high molecular weight.
    • 在由包含过渡金属络合物的缩合剂共存的情况下,使由式(1)表示的单体或由式(1)表示的单体与式(2)表示的单体共聚的方法, 从而制备由式(3)表示的高分子化合物:X1-Ar1-X2(1)X3-Ar2-X4(2) - (Ar1)q-(Ar2)r-(3)[X1,X2,X3和 X 4表示在缩合中分离的基团,Ar 1表示通过连接基团作为取代基具有至少具有磺酸或磺酸的2价芳香族基团,q表示正数,r表示0或正数, q和r的和为300以上],其特征在于,上述缩合剂和上述单体在45℃以上的温度下混合。 上述方法允许制备显示出优异的燃料电池特性并且具有高分子量的高分子化合物。