    • 61. 发明授权
    • Bimodal polyethylene resins that have high stiffness and high ESCR
    • 具有高刚度和高ESCR的双峰聚乙烯树脂
    • US08138264B2
    • 2012-03-20
    • US11744596
    • 2007-05-04
    • Tim J. CoffyGerhard GuentherSteven D. Gray
    • Tim J. CoffyGerhard GuentherSteven D. Gray
    • C08F4/642C08F210/16
    • C08F10/02C08F110/02C08F210/16C08F4/6555C08F2/001C08F2500/05C08F2500/13C08F2500/07C08F2500/11C08F2500/12C08F210/08
    • A bimodal polyethylene having a high density ranging from about 0.955 to about 0.959 g/cc, an improved environmental stress cracking resistance (ESCR) of from about 400 to about 2500 hours, and an improved 0.4% flexural modulus of from about 180,000 to about 260,000 psi (1,200 MPa to about 1,800 MPa) may be formed using a Ziegler-Natta polymerization catalyst using two reactors in series. The bimodal polyethylene may have a high load melt index (HLMI) of from about 2 and about 30 dg/min and may be optionally made with a small amount of alpha-olefinic comonomer in the second reactor. It is emphasized that this abstract is provided to comply with the rules requiring an abstract which will allow a searcher or other reader to quickly ascertain the subject matter of the technical disclosure. It is submitted with the understanding that it will not be used to interpret or limit the scope or meaning of the claims.
    • 具有约0.955至约0.959g / cc的高密度的双峰聚乙烯,约400至约2500小时的改进的耐环境应力开裂性(ESCR)和约180,000至约260,000的改善的0.4%挠曲模量 可以使用串联的两个反应器的齐格勒 - 纳塔聚合催化剂形成psi(1200MPa至约1800MPa)。 双峰聚乙烯可以具有约2和约30dg / min的高负载熔体指数(HLMI),并且可以任选地在第二反应器中用少量的α-烯烃共聚单体制备。 要强调的是,该摘要被提供以符合要求摘要的规则,这将允许搜索者或其他读者快速确定技术公开的主题。 提交它的理解是,它不会用于解释或限制权利要求的范围或含义。
    • 64. 发明申请
    • Polymerization process providing polyethylene of enhanced optical properties
    • 提供增强光学性能的聚乙烯的聚合方法
    • US20080269441A1
    • 2008-10-30
    • US11796888
    • 2007-04-30
    • Gerhard GuentherDavid W. KnoeppelSteven D. GrayTim J. Coffy
    • Gerhard GuentherDavid W. KnoeppelSteven D. GrayTim J. Coffy
    • C08F4/44
    • C08F10/00C08F210/16C08F4/69C08F2/14C08F210/14C08F2500/12
    • A process for the polymerization of ethylene to provide an ethylene polymer of reduced Yellowness Index. A feed stream, comprising an inert hydrocarbon diluent containing ethylene in a minor amount, is supplied to a polymerization reactor. A chromium-based polymerization catalyst and a triethylboron co-catalyst are incorporated into the feed stream within the reactor. The polymerization catalyst will normally be used in an amount within the range of 0.008-0.1 wt. % of the diluent in the feed stream and the triethylboron co-catalyst is incorporated in an amount within the range of 0.1-50 ppm of the diluent. The polymer fluff from the reactor is heated to a temperature sufficient to melt the fluff which is then extruded to produce a polymer product. The Yellowness Index after high temperature aging is at least 5% less than the corresponding Yellowness Index of a corresponding polymer product produced without the triethylboron co-catalyst.
    • 一种聚合乙烯以提供降低黄度指数的乙烯聚合物的方法。 将包含少量乙烯的惰性烃稀释剂的进料流供给到聚合反应器中。 在反应器内的进料流中加入铬基聚合催化剂和三乙基硼助催化剂。 聚合催化剂通常的用量范围为0.008-0.1wt。 进料流和三乙基硼助催化剂中稀释剂的%的掺入量在稀释剂的0.1-50ppm的范围内。 将来自反应器的聚合物绒毛加热到足以熔化绒毛的温度,然后将其挤出以产生聚合物产物。 高温老化后的黄度指数比没有三乙基硼助催化剂生产的相应的聚合物产物的相应黄度指数小至少5%。