    • 48. 发明授权
    • Method for curing fluoropolymer
    • 含氟聚合物固化方法
    • US06835782B1
    • 2004-12-28
    • US10030914
    • 2002-01-14
    • Shigeru MoritaTakuya AraseTetsuo Shimizu
    • Shigeru MoritaTakuya AraseTetsuo Shimizu
    • C08F832
    • C08F8/00C08F14/18
    • A polymer having a structure of the formula: in which X, Y and Z represent independently each other H, F, Cl, Br or I, provided that at least one of X, Y and Z is F; R represents a straight or branched fluorinated alkylene group which may contain an oxygen atom; x and y represent mole percentages and x is from 1 to 100% by mole; A is —CN, —NCO, —COOR′ in which R′ is H or an alkyl group having 1 to 10 carbon atoms, an acid anhydride group or an unsaturated hydrocarbon group; and M is a repeating unit derived from a copolymerizable monomer is treated with a crosslinking agent selected from ammonia, diamines and polyol compounds and crosslinked through the side functional groups of the polymer. This crosslinking method can be carried out at room temperature and provides a transparent fluoropolymer having better heat resistance than conventional transparent thermoplastic resins.
    • 具有以下结构的聚合物:其中X,Y和Z彼此独立地表示H,F,Cl,Br或I,条件是X,Y和Z中的至少一个为F; R表示可以含有氧原子的直链或支链氟化亚烷基; x和y表示摩尔百分比,x为1〜100摩尔% A是-CN,-NCO,-COOR',其中R'是H或具有1-10个碳原子的烷基,酸酐基或不饱和烃基; M是来自可共聚单体的重复单元,用选自氨,二胺和多元醇化合物的交联剂进行处理,并通过聚合物的侧官能团交联。 该交联方法可以在室温下进行,并提供与常规的透明热塑性树脂相比具有更好的耐热性的透明含氟聚合物。
    • 50. 发明授权
    • Polyphenylene sulfide resin compositions and process for preparation of
same
    • 聚苯硫醚树脂组合物及其制备方法
    • US5684088A
    • 1997-11-04
    • US412592
    • 1995-03-29
    • Tsuyoshi MiyamoriYoshihisa YamamotoMasami KatoMasaji KomoriTetsuo Shimizu
    • Tsuyoshi MiyamoriYoshihisa YamamotoMasami KatoMasaji KomoriTetsuo Shimizu
    • C08L27/18C08L81/02C08G63/48C08L81/00
    • C08L81/02C08L27/18Y10S525/902
    • The present invention relates to a PPS resin composition comprising a matrix of the PPS which is filled with a PTFE powder baked at a temperature not less than a melting point thereof and having a number-average molecular weight of not less than 1.5 million or PTFE fine particles having an average particle size of 0.05 to 1 .mu.m and comprising a fibrillating core portion of a high molecular weight PTFE with a number-average molecular weight of not less than 1.5 million and a non-fibrillating shell portion of a low molecular weight PTFE so that a content thereof is 40 to 80% by weight in the composition, and also relates to a process for preparing said PPS resin composition, which is characterized in that melting and kneading are carried out at a temperature from a temperature of not less than a melting point of PPS to a temperature of not more lower than a melting point of a high molecular weight PTFE. The polyphenylene sulfide resin composition of the present invention presents sliding properties such as excellent friction and wear resistance which sliding materials mainly containing usual polytetrafluoroethylene have as well as properties of polyphenylene sulfide such as injection moldability and high mechanical properties.
    • 本发明涉及一种PPS树脂组合物,其包含PPS基体,其填充有在不低于其熔点的温度下焙烧的数均分子量不小于150万的PTFE粉末或PTFE细粉 平均粒径为0.05-1μm的颗粒,其包含数均分子量不小于150万的高分子量PTFE的原纤化核心部分和低分子量PTFE的非原纤化壳部分 使其含量在组合物中为40〜80重量%,并且还涉及制备所述PPS树脂组合物的方法,其特征在于熔融和捏合在不低于 PPS的熔点至不高于高分子量PTFE的熔点的温度。 本发明的聚苯硫醚树脂组合物具有优异的摩擦和耐磨性的滑动性能,主要含有通常的聚四氟乙烯的滑动材料以及聚苯硫醚的性能如注射成型性和高机械性能。