    • Method for preparing particles with a conjugated polymer shell
    • Verfahren zur Herstellung von Partikeln mit einerPolymerkonjugathülle
    • EP2246376A1
    • 2010-11-03
    • EP09005837.1
    • 2009-04-27
    • Leibniz-Institut für Polymerforschung Dresden e.V.
    • Kiriy, AntonSenkovskyy, VolodymyrStamm, Manfred
    • C08F292/00C08F291/00C08F257/02C08F259/00C08F277/00C08F285/00C08F271/02C08G83/00C08L65/02C08G61/02
    • C08F292/00C08F257/02C08F259/00C08F271/02C08F277/00C08F285/00C08F291/00C08L51/003C08L51/08C08L51/085C08L51/10C08L2666/02
    • The invention is directed to a method for preparing hybrid particles comprising the steps of:
      a) providing particles having a plurality of-Ar 1 -X groups on their surface,
      b) preparing initiated sites -Ar 1 -NiL-X on the surface of the particles from step a) using a Ni(II) or Ni(0) compound,
      c) contacting the particles from step b) with propagation monomers of the general formula Z-Ar 2 -X to form polymer chains attached to the particles,

      wherein
      Ar 1 and Ar 2 are independently selected from substituted or unsubstituted aryl or heteroaryl groups,
      L represents two monodentate ligands which are selected from the group consisting of triarylphosphine (PAr 3 ), trialkylphosphine (PR 3 ) and combinations thereof; or L represents a bidentate ligand which is selected from the group consisting of 2,2'-bipyridyl (bipy), α-N,N'-diaryl-acenaphthenediimine (daadi), [1,3-bis(diphenylphosphino) propane] (dppp), 1,2-bis(diphenylphosphino)ethane (dppe), [1,1'-bis(diphenylphosphino)ferrocene] (dppf), and combinations thereof;
      Z is XMg, XZn or Li;
      X is a halogen.
      The invention is further directed to hybrid particles obtainable by this method and the use of the hybrid particles in optoelectronic, sensor and solar cell applications, and to the solar cell itself.
    • 本发明涉及一种制备杂化颗粒的方法,包括以下步骤:a)在其表面上提供具有多个Ar 1 -X基团的颗粒,b)在表面上制备起始位点-Ar 1 -NiL-X 来自步骤a)的使用Ni(II)或Ni(0)化合物的颗粒,c)使来自步骤b)的颗粒与通式Z-Ar 2 -X的传播单体接触以形成附着于颗粒的聚合物链, 其中Ar 1和Ar 2独立地选自取代或未取代的芳基或杂芳基,L表示选自三芳基膦(PAr 3),三烷基膦(PR 3)及其组合的两个单齿配体; 或L表示选自2,2'-联吡啶(bipy),±-N,N'-二芳基 - 苊基亚胺(daadi),[1,3-双(二苯基膦基)丙烷]( dppp),1,2-双(二苯基膦基)乙烷(dppe),[1,1'-双(二苯基膦基)二茂铁](dppf)及其组合; Z是XMg,XZn或Li; X是卤素。 本发明还涉及通过该方法获得的混合颗粒和在光电子,传感器和太阳能电池应用中使用混合颗粒以及太阳能电池本身。