    • 36. 发明授权
    • Polyimide composition
    • 聚酰亚胺组合物
    • US5321096A
    • 1994-06-14
    • US35043
    • 1993-03-22
    • Yuichi OkawaNobuhito KogaHideaki OikawaTadashi AsanumaAkihiro Yamaguchi
    • Yuichi OkawaNobuhito KogaHideaki OikawaTadashi AsanumaAkihiro Yamaguchi
    • C08G73/10C08L71/00C08L79/08C08L81/06C08F283/04C08G69/48
    • C08L71/00C08G73/101C08L79/08C08L81/06
    • A thermoplastic resin composition comprise 99.9.about.50 parts by weight of one or more thermoplastic resin selected from the group consisting of aromatic polyimide, aromatic polyetherimide, aromatic polyamideimide, aromatic polyethersulfone and aromatic polyether ketone and 0.1.about.50 parts by weight of one or more liquid crystal type aromatic polyimide having recurring structural units represented by the formula (1): ##STR1## wherein R.sub.1 .about.R.sub.5 is a hydrogen atom, fluorine atom, trifluoromethyl, methyl, ethyl or cyano and may be the same or different, and R is a tetravalent radical having 6.about.27 carbon atoms and being selected from the group consisting of a monoaromatic radical, condensed polyaromatic radical and noncondensed aromatic radical connected each other with a direct bond or a bridge member.The present invention can provide thermoplastic resin compositions which have remarkably good processability and excellent thermal stability in addition to essentially excellent properties of each resin.
    • 热塑性树脂组合物包含99.9重量份的一种或多种选自芳族聚酰亚胺,芳族聚醚酰亚胺,芳族聚酰胺酰亚胺,芳族聚醚砜和芳族聚醚酮的热塑性树脂和0.1重量份的一种或多种液体 具有由式(1)表示的重复结构单元的结晶型芳族聚酰亚胺:(1)n原子,氟原子,三氟甲基,甲基,乙基或氰基,可以相同或不同,R是具有 6个碳原子,并且选自由直链或桥构件相互连接的单芳族基团,缩合多芳族基团和非缩合芳族基团组成的组。 本发明可以提供具有非常好的加工性和优异的热稳定性的热塑性树脂组合物,除了每种树脂的基本上优异的性能。
    • 38. 发明授权
    • Polyimide resin composition
    • 聚酰亚胺树脂组合物
    • US6103806A
    • 2000-08-15
    • US216867
    • 1998-12-21
    • Hiroyasu KidoMasaji YoshimuraYasunori YoshidaKayako YanagiharaHideaki OikawaShoji TamaiTomohito Koba
    • Hiroyasu KidoMasaji YoshimuraYasunori YoshidaKayako YanagiharaHideaki OikawaShoji TamaiTomohito Koba
    • C08L79/08
    • C08L79/08
    • A polyimide resin composition is disclosed herein which comprises 5 to 60% by weight of a polyimide [polyimide (1)] having a repeating unit represented by the chemical formula 1 and 40 to 95% by weight of a polyimide [polyimide (2)] having a repeating unit represented by the chemical formula 2. According to the present invention, there are provided a polymer alloy in which the advantages of the polyimide (1) and the polyimide (2) are utilized and the disadvantages of the polyimide (1) and the polyimide (2) are reduced; a polyimide resin composition from which crystalline molded articles can be obtained even by a usual molding cycle, for example, an injection molding cycle of about 30 to 60 seconds; and a polyimide resin composition from which molded articles having an excellent dimensional accuracy and flexural modulus can be obtained even by a usual molding cycle, for example, an injection molding cycle of about 30 to 60 seconds, for example, in the case that the molded articles are intended to be used at a high temperature of 230.degree. C. or more, for example, a temperature of 230 to 300.degree. C., or 230 to 250.degree. C.
    • 本文公开了一种聚酰亚胺树脂组合物,其包含5至60重量%的具有由化学式1表示的重复单元的聚酰亚胺[聚酰亚胺(1)]和40至95重量%的聚酰亚胺[聚酰亚胺(2)] 具有由化学式2表示的重复单元。根据本发明,提供了使用聚酰亚胺(1)和聚酰亚胺(2)的优点的聚合物合金,并且聚酰亚胺(1) 并且聚酰亚胺(2)被还原; 聚酰亚胺树脂组合物,甚至可以通过通常的成型周期获得结晶模制品,例如约30至60秒的注塑周期; 以及聚酰亚胺树脂组合物,即使在通常的成型周期(例如,注射成型周期为约30〜60秒)下,也可以获得具有优异的尺寸精度和挠曲模量的成型制品,例如在成型 制品应在230℃或更高的高温下使用,例如温度为230-300℃,或230-250℃。
    • 39. 发明授权
    • Automatic lead advance for mechanical pencils
    • 铅笔铅笔自动提前
    • US4838721A
    • 1989-06-13
    • US188814
    • 1988-04-29
    • Hideaki Oikawa
    • Hideaki Oikawa
    • B43K21/033
    • B43K21/033
    • An automatic lead advance for a mechanical pencil having a tubular casing, a conical member joined to the front end portion of the tubular casing, a ring fixed to the inner surface of the conical member, an annular pivotable member provided at the front side of the ring, a lead guide tube having a lead retainer, urged backward by a spring, adapted to the slidable in the axial direction, and positioned so that the portion of the front end surface of the pivotable member which is away from the fulcrum of pivotal movement thereof contacts the rear end portion of the lead guide tube, a ball chuck mechanism urged forward by a knock spring and adapted to be movable between the rear end surface of the ring and an end surface of a stepped portion formed on the inner surface of the tubular casing, and a stopper provided at the front end of an outer tube of the ball chuck mechanism and contacting at the front end surface thereof the portion of the rear end surface of the pivotable member which is close to the fulcrum of pivotal movement thereof.
    • 一种用于具有管状壳体的自动铅笔的自动引线提前,连接到管状壳体的前端部分的圆锥形构件,固定到锥形构件的内表面的环,设置在管状壳体的前侧的环形可枢转构件 环,具有引线保持器的引导引导管,其被弹簧向后推动,适于在轴向方向上可滑动,并且定位成使得可枢转构件的前端表面远离枢转运动的支点的部分 其接触引导引导管的后端部,由卡止弹簧向前推动的球卡盘机构,其适于在环的后端面与形成于所述引导导管的内表面的阶梯部的端面之间移动 管状壳体和设置在球卡盘机构的外管的前端的止动件,并在其前端面处接触可枢转构件的后端面的部分,其中i 靠近其枢轴运动的支点。