    • 2. 发明授权
    • Field emission display and method of manufacture
    • 场发射显示及制造方法
    • US06716078B1
    • 2004-04-06
    • US09626979
    • 2000-07-27
    • Matthew StainerShawn M. O'RourkeKazuo KatoSusumu Sakamoto
    • Matthew StainerShawn M. O'RourkeKazuo KatoSusumu Sakamoto
    • H01J9227
    • H01J9/2271H01J29/085
    • A field emission display (30) having an anode plate (10) that has phosphor channels (13, 14, 15). The phosphor channels (13, 14, 15) are formed by depositing a first layer of photosensitive film (58) on a substrate (11). Stripes are patterned into the first layer photosensitive film (58) using ultraviolet light. A second layer of photosensitive film (59) is formed on the first layer of photosensitive film (58). Stripes are patterned into the second layer of photosensitive film (59) using ultraviolet light. The stripes in the second layer of photosensitive film (58) are substantially perpendicular to the first layer of photosensitive film (59). Both layers of photosensitive film are developed to form channel structures. Phosphor is formed in the channel structures to form the phosphor channels (13, 14, 15). The anode plate (10) is coupled to a cathode plate (31) to form the field emission display (30).
    • 具有具有荧光体通道(13,14,15)的阳极板(10)的场致发射显示器(30)。 荧光体通道(13,14,15)通过在基板(11)上沉积第一层感光膜(58)而形成。 使用紫外线将条纹图案化成第一层感光膜(58)。 在第一感光膜(58)上形成第二层感光膜(59)。 使用紫外光将条纹图案化成第二层感光膜(59)。 感光膜(58)的第二层中的条纹基本上垂直于第一层感光膜(59)。 开发两层感光膜以形成通道结构。 在沟道结构中形成荧光体以形成荧光体通道(13,14,15)。 阳极板(10)连接到阴极板(31)以形成场致发射显示器(30)。
    • 4. 发明申请
    • Methods for Attaching Flexible Substrates to Rigid Carriers and Resulting Devices
    • 将柔性基板连接到刚性载体和结果装置的方法
    • US20110311789A1
    • 2011-12-22
    • US13062020
    • 2009-09-10
    • Douglas E. LoyShawn M. O'Rourke
    • Douglas E. LoyShawn M. O'Rourke
    • B23K31/02B32B3/22
    • H01L21/6835H01L2221/6835H05K1/0393H05K3/007H05K3/341Y10T428/24826
    • Flexible substrates can be temporarily attached to a rigid carrier for processing a surface thereof by depositing a joining material at one or more contact points between a flexible substrate and a rigid carrier, contacting the flexible substrate and the rigid carrier at the one or more contact points; and exposing the one or more contact points to a temperature of between 219° C. and 1000° C. and under conditions suitable for attaching the flexible substrate and the rigid carrier at the one or more contact points via the joining material. Examples of suitable joining materials include, but are not limited to soldering or brazing materials. Such supported substrates can be used for preparing flexible displays comprising at least one electronic component and/or circuit on a surface of the flexible display.
    • 柔性基底可以临时附接到刚性载体上,以通过在柔性基底和刚性载体之间的一个或多个接触点处沉积接合材​​料来处理其表面,在柔性基底和刚性载体之间,在一个或多个接触点 ; 以及将所述一个或多个接触点暴露于介于219℃和1000℃之间的温度下,以及适于通过所述接合材料在所述一个或多个接触点附接所述柔性基底和所述刚性载体的条件。 合适的接合材料的实例包括但不限于焊接或钎焊材料。 这种支撑的基底可以用于制备在柔性显示器的表面上包括至少一个电子部件和/或电路的柔性显示器。
    • 5. 发明授权
    • Viewing screen for a display device
    • 查看显示设备的屏幕
    • US06400072B1
    • 2002-06-04
    • US09520911
    • 2000-03-08
    • Shawn M. O'RourkeNick R. MunizzaMatthew Stainer
    • Shawn M. O'RourkeNick R. MunizzaMatthew Stainer
    • H01J2910
    • H01J29/085H01J9/2278
    • A viewing screen (100) for a display device (115) includes a glass substrate (110) having a thermal coefficient of expansion within a range of 3.5×10−6−4.5×10−6 °C.−1. Viewing screen (100) further includes a black matrix (111), which is affixed to glass substrate (110), and which includes a black surround, a ductile metal, and lead titanate. A method for fabricating viewing screen (100) includes the steps of: adding to a black surround paste a ductile metal paste, adding to the black surround paste lead titanate particles, depositing the black surround paste on glass substrate (110), and heating the black surround paste and glass substrate (110) to affix the black surround paste to glass substrate (110), thereby forming black matrix (111). The ductile metal paste and lead titanate particles are added in amounts sufficient to realize an extent of cracking in black matrix (111) upon repeated heating to a temperature within a range of 450-600° C. that is significantly less than that exhibited by an unimproved black matrix, which is made only from the material of the black surround paste.
    • 用于显示装置(115)的观察屏(100)包括具有在3.5×10-6-4.5×10 -6℃-1范围内的热膨胀系数的玻璃基板(110)。 观看屏幕(100)还包括固定在玻璃基板(110)上的黑色矩阵(111),其包括黑色环绕部分,延性金属和钛酸铅。1.一种用于制造观察屏幕(100)的方法,包括: 步骤:向黑色环绕糊料中加入延性金属糊料,加入黑色环绕糊状钛酸铅颗粒,将黑色环绕糊剂沉积在玻璃基板(110)上,并加热黑色环绕糊状物和玻璃基板(110)以贴附 黑色环绕糊状物到玻璃基板(110),由此形成黑色矩阵(111)。 延展性金属糊料和钛酸铅颗粒的添加量足以在反复加热至450-600℃范围内的温度下实现黑色矩阵(111)中的开裂程度,这显着小于由 未经改进的黑色矩阵,仅由黑色环绕糊的材料制成。
    • 6. 发明授权
    • Viewing screen for a display device and method for the fabrication thereof
    • 显示装置的观看屏幕及其制造方法
    • US06660324B2
    • 2003-12-09
    • US10123765
    • 2002-04-16
    • Shawn M. O'RourkeNick R. MunizzaMatthew Stainer
    • Shawn M. O'RourkeNick R. MunizzaMatthew Stainer
    • B05D500
    • H01J29/085H01J9/2278
    • A method for fabricating viewing screen (100) includes the steps of: adding to a black surround paste a ductile metal paste, adding to the black surround paste lead titanate particles, depositing the black surround paste on glass substrate (110), and heating the black surround paste and glass substrate (110) to affix the black surround paste to glass substrate (110), thereby forming black matrix (111). The ductile metal paste and lead titanate particles are added in amounts sufficient to realize an extent of cracking in black matrix (111) upon repeated heating to a temperature within a range of 450-600° C. that is significantly less than that exhibited by an unimproved black matrix, which is made only from the material of the black surround paste.
    • 一种用于制造观察屏(100)的方法包括以下步骤:向黑色环绕糊状物添加延性金属浆料,将黑色环绕糊状铅酸铅颗粒添加到玻璃基板(110)上,并将黑色环绕糊料沉积在玻璃基板 黑色环绕糊状物和玻璃基板(110),以将黑色环绕糊状物贴合到玻璃基板(110)上,从而形成黑色矩阵(111)。 延展性金属糊料和钛酸铅颗粒的添加量足以在反复加热至450-600℃范围内的温度下实现黑色矩阵(111)中的开裂程度,这显着小于由 未经改进的黑色矩阵,仅由黑色环绕糊的材料制成。