基本信息:
- 专利标题: 저 OH, OD 수준을 갖는 융합 실리카 및 그 제조방법
- 专利标题(英):Fused silica having low oh, od levels and method of making
- 专利标题(中):具有低OH,熔点和制备方法的熔融二氧化硅
- 申请号:KR1020107004705 申请日:2008-07-18
- 公开(公告)号:KR1020100058525A 公开(公告)日:2010-06-03
- 发明人: 크라프코,로스티슬라프알 , 레브론드,니콜라스 , 틴글리,제임스이
- 申请人: 코닝 인코포레이티드
- 申请人地址: One Riverfront Plaza, Corning, NY ***** U.S.A.
- 专利权人: 코닝 인코포레이티드
- 当前专利权人: 코닝 인코포레이티드
- 当前专利权人地址: One Riverfront Plaza, Corning, NY ***** U.S.A.
- 代理人: 청운특허법인
- 优先权: US11/881,599 2007-07-27
- 国际申请: PCT/US2008/008836 2008-07-18
- 国际公布: WO2009017613 2009-02-05
- 主分类号: C03B19/14
- IPC分类号: C03B19/14 ; C03C3/06
摘要:
A fused silica article having a combined concentration of hydroxyl and deuteroxyl concentration of less than 10 parts per million (ppm) and, in one embodiment, less than 1 ppm. The fused silica article is formed by drying a soot blank in a halogen-free atmosphere comprising carbon monoxide. The dried soot blank may optionally be doped to reach target levels of OH and OD concentrations and improve homogeneity within the fused silica article. The dried soot blank is then oxidized and sintered to form the article. A method of reducing the combined concentration of OH and OD to less than 10 ppm is also described.
摘要(中):
具有小于10ppm(ppm)的羟基和氘氧化物浓度的组合浓度的熔融二氧化硅制品,在一个实施方案中小于1ppm。 熔融二氧化硅制品通过在包含一氧化碳的无卤素气氛中干燥烟炱坯料而形成。 干燥的烟炱坯料可以任选地被掺杂以达到OH和OD浓度的目标水平并且改善熔融二氧化硅制品内的均匀性。 然后将干燥的烟灰坯料氧化并烧结以形成制品。 还描述了将OH和OD的组合浓度降低至小于10ppm的方法。
公开/授权文献:
- KR101504377B1 저 OH, OD 수준을 갖는 융합 실리카 및 그 제조방법 公开/授权日:2015-03-19