    • METHOD FOR PRODUCING A MOULDED PART
    • 用于生产组成部分
    • WO2004012885A3
    • 2004-10-21
    • PCT/AT0300217
    • 2003-07-30
    • PLANSEE AGZOBL GEBHARDGLATZ WOLFGANGKRAUSSLER WOLFGANGOBERBREYER ROBERT
    • ZOBL GEBHARDGLATZ WOLFGANGKRAUSSLER WOLFGANGOBERBREYER ROBERT
    • B22F3/02B22F5/00H01M8/02H01M8/0208H01M8/0215H01M8/0247
    • B22F3/164B22F3/02B22F5/00B22F2998/00B22F2998/10H01M8/0208H01M8/0215H01M8/0247Y02E60/50C22C33/0207H01M8/02B22F3/10
    • The invention relates to a method for producing a moulded part from a disk-shaped or plate-shaped base body (5) comprising a plurality of knot-shaped and/or ridge-shaped elevations (4, 3) which merge into the base body (5) with inclined lateral surfaces, by pressing and sintering powdery starting materials into a shape that is close to the end shape. According to the invention, the pressing takes place in a two-step pressing process. In the first pressing step, the defining surfaces of the base body (5) are pressed up to the elevations (3, 4), in order to form an at least approximate end shape, and the elevations (3, 4) are simultaneously pressed with overdimension. The projection h of the elevations (3, 4) in relation to the base body (5) is 10 % to 150 % higher than the projection h' in the finished pressed state. The lateral surfaces form an angle of inclination alpha ' between 90 DEG and 150 DEG with the respectively adjacent defining surface of the base body (5). In the second pressing step, the elevations (3, 4) are pressed to form an at least approximate end shape, the angle of inclination
    • 本发明涉及一种方法,用于生产圆盘或板形的基体(5)的与多个knob-和/或网络状凸起形成的成型体(4,3)设置有倾斜侧面到基体(5)通过由接近最终形状的加压和 烧结粉末状的原料。 根据本发明,在两阶段的按压操作的按压。 在第一按压阶段的基体(5)的对调查的边界表面(3,4)朝向至少压制成近净形状,并且凸部(3,4)同时用过量的按压。 将上清液H“的突起(3,4)从所述基体(5)是投影ħ”相对10%的成品按压状态 - 更大的150%。 其侧面包括一个倾斜角度阿尔法“中的90°的范围内 - 150°与基体(5)的相应的相邻的边界表面。 170℃ - 在第二冲压工序中,突出部(3,4)至少近净形状,其中倾斜的α“与α的值的角度为95°的范围内增加的按压。