    • 1. 发明申请
    • METHOD FOR MANUFACTURING A PRODUCT IN SULPHUR CONCRETE AND DEVICE APPLIED THEREIN
    • 硫磺混凝土制品的制造方法及其装置
    • WO2018069862A1
    • 2018-04-19
    • PCT/IB2017/056319
    • 2017-10-12
    • THIO MATERIALS, BESLOTEN VENNOOTSCHAP MET BEPERKTE AANSPRAKELIJKHEID
    • DE BONTE, Filip
    • B28B1/34B28B7/42B28B21/30B28B21/78C04B28/36B28B1/54
    • B28B21/78B28B1/34B28B1/54B28B7/42B28B21/30C04B28/36C04B40/0085
    • Method for the manufacture of a product of sulphur concrete with the steps: - the heating of a mixture of sulphur concrete (21) to above melting temperature; ⋅- the provision of a mould (9) that is driven around its axis (X-X'); ⋅- the heating of the rotating mould (9) to a temperature above the melting temperature of sulphur; ⋅- the simultaneous addition of liquid sulphur concrete (21); ⋅- when the layer of liquid sulphur concrete (28) has reached a certain thickness (A), the stopping of heating and start of cooling the rotating mould (9) from the outside while the inside space (30) of the drum (9) is kept at a temperature that is higher than the melting temperature of the sulphur; ⋅- if required, further cooling of the mould from the outside and the gradual further supply of heated liquid sulphur concrete until the necessary quantity of sulphur concrete (21) to form the product (1) has been reached and until the sulphur (21) concrete has sufficiently hardened;
    • 通过以下步骤制造硫磺混凝土产品的方法: - 将硫磺混凝土(21)的混合物加热至熔融温度以上; ⋅-提供围绕其轴线(X-X')驱动的模具(9); ·将旋转模具(9)加热到高于硫的熔化温度的温度; ⋅-同时加入液态硫磺混凝土(21); ·当液硫混凝土层28达到一定厚度(A)时,停止加热并开始从外部冷却旋转模具(9),同时使滚筒(9)的内部空间(30) )保持在高于硫的熔化温度的温度下; ⋅如果需要,从外部进一步冷却模具,并逐渐进一步供应加热的液态硫混凝土,直到达到形成产品(1)的必要数量的硫磺混凝土(21),并且直到硫(21) 混凝土已经充分硬化;