    • BUTTERFLY WING LAMINATION PROCESS AND METHOD OF USE
    • WO2005000492A3
    • 2005-03-10
    • PCT/US2004017851
    • 2004-06-04
    • SOUKUP MICHAEL
    • SOUKUP MICHAEL
    • A01N1/00B21B20060101B29C70/54B29C70/68B44C5/06
    • B29C70/685B29C70/545B29K2063/00B29L2031/7434B44C5/06Y10T156/1057
    • A multi-layer lamination process for butterfly wings to facilitate their use in jewelry, accessories, gift items and the like is disclosed. The process includes the steps of mixing of a liquid epoxy resin (110), application of a layer of the liquid epoxy resin to a sheet of polyester film (115), affixing a butterfly wing to the liquid epoxy resin/polyester film combination (120), allowing the layer of epoxy resin to dry (125), applying a layer of fixative to the exposed side of the butterfly wing (130), allowing the layer of fixative to dry (135), applying a first layer of clear lacquer/resin over the fixative (140), allowing the first layer of lacquer/resin to dry (145), cutting along the outer perimeter of the butterfly wing to separate the wing from the remainder of the polyester film (150), smoothing out the edges of the cut-out butterfly wing (155), application of a second layer of clear lacquer/resin over the first layer (160), allowing the second layer of lacquer/resin to dry (165), application of a third layer of lacquer/resin over the second layer (170), and allowing the third layer of lacquer/resin to dry (175).
    • 公开了一种用于蝴蝶翅膀以便于其在珠宝,配件,礼物等中的使用的多层层压方法。 该方法包括以下步骤:将液体环氧树脂(110)混合,将液体环氧树脂层施加到聚酯薄膜片(115)上,将蝴蝶翼固定在液体环氧树脂/聚酯薄膜组合(120 ),允许环氧树脂层干燥(125),将一层固定剂施加到蝴蝶翼(130)的暴露侧,允许固定剂层干燥(135),施加第一层透明漆/ 树脂在固定剂(140)上方,允许第一层漆/树脂干燥(145),沿着蝴蝶翼的外周切割以将翼与聚酯膜(150)的其余部分分离,从而平滑边缘 的切割蝴蝶翼(155),在第一层(160)上施加第二层清漆/树脂,允许第二层漆/树脂干燥(165),施加第三层漆 /树脂在第二层(170)上,并且允许第三层漆/树脂干燥(175)。
    • 4. 发明申请
    • BUTTERFLY WING LAMINATION PROCESS AND METHOD OF USE
    • WO2005000492A2
    • 2005-01-06
    • PCT/US2004/017851
    • 2004-06-04
    • SOUKUP, Michael
    • SOUKUP, Michael
    • B21B
    • B29C70/685B29C70/545B29K2063/00B29L2031/7434B44C5/06Y10T156/1057
    • A multi-layer lamination process for butterfly wings to facilitate their use in jewelry, accessories, gift items, crafts, etc. The process steps include (1) the mixing of a liquid epoxy resin, (2) application of a layer of the liquid epoxy resin to a sheet of Mylar® (3) affixing a butterfly wing to the liquid epoxy resin/Mylar® sheet combination, (4) allowing the layer of liquid epoxy resin to dry, (5) applying a layer of fixative to the exposed side of the butterfly wing, (6) allowing the layer of fixative to dry, (7) applying a first layer of clear lacquer/resin over the fixative, (8) allowing the first layer of lacquer/resin to dry, (9) cutting along the outer perimeter of the butterfly wing to separate the wing from the remainder of the Mylar® sheet, (10) smoothing the edges of the cut-out butterfly wing, (11) the application of a second layer of clear lacquer/resin over the first layer, (12) allowing the second layer of lacquer/resin to dry, (13) applying a third layer of clear lacquer/resin over the second layer, and (14) allowing the third layer of lacquer/resin to dry. In addition, a hole may be drilled through one end of the laminated butterfly wing, and a bail affixed to the hole for jewelry design. The process results in a multi-layered lamination that strengthens and preserves the wing's naturally occurring colors and patterns.
    • 用于蝴蝶翅膀的多层层压方法,以便于其在珠宝,配件,礼品,工艺品等中的使用。工艺步骤包括(1)液体环氧树脂的混合,(2)施加一层液体 环氧树脂粘合到将液体环氧树脂/聚酯薄片组合固定蝴蝶翼的Mylar(3)片材上,(4)允许液体环氧树脂层干燥,(5)施加一层 固定在蝴蝶翼的暴露面上,(6)允许固定剂层干燥,(7)在固定剂上施加第一层清漆/树脂,(8)允许第一层漆/树脂干燥 ,(9)沿蝴蝶翼的外周切割以将翼与Mylar(R)片的其余部分分开,(10)使切割的蝴蝶翼的边缘平滑,(11)应用第二 在第一层上的透明漆/树脂层,(12)允许第二层漆/树脂干燥,(13)施加第三层cl 耳漆/树脂在第二层上,和(14)允许第三层漆/树脂干燥。 另外,可以通过层叠蝴蝶翼的一端钻出一个孔,并将一个保护环固定在孔上用于珠宝设计。 该过程产生了多层层压,其加强并保持机翼的天然存在的颜色和图案。
    • 5. 发明申请
    • PROCESS OF MANUFACTURING TROPHIES, MEDALS AND AWARD PLATES, MADE OF POLYESTER, ESTERVINYLIC OR EPOXY RESINS, REINFORCED WITH FIBERGLASS
    • 制造TROPHIES,MEDALS和AWARD PLATES的方法,用FIBERGLASS加固的聚酯,环氧树脂或环氧树脂
    • WO99032006A2
    • 1999-07-01
    • PCT/BR1998/000113
    • 1998-12-14
    • A44C27/00B32B37/00B44C5/00B44C5/04B44F1/06A44C
    • B44F1/06A44C27/00B29C70/086B29C70/088B29C70/30B29K2105/06B29L2031/7434B44C5/00B44C5/0423B44C5/0446Y10T156/108
    • The present patent is characterized by enlarging the use of polyester, estervinylic and epoxy resins, reinforced with fiberglass, utilizing them as inviolately involucre in plain, spherical, cylindrical or another geometrical form, to polychromies made in transparencies, papers, cloths, plastics, wood, metals, leather, et al; generated by computer, manually or by any other kind of printing. Its production incorporates: one or more dismolder layers on glassy or polished base; one or more catalysed resin layer over the dismolder; one or more woven forms, textile forms, or roving forms fiberglass layers; insertion, in the laminate, of polychromies in transparency, paper, cloth, wood, metal or leather, containing characters, drawings, paintings, pictures, photographies, signatures, et al; generated by computer, manually or by any other kind of printing; one or more cloth layers; one or more woven forms, textile forms, or roving forms fiberglass layers; one or more resin layers; application of plastic film; rouletting and retreat of bubbles; dismold. The polychromies of the laminate, being cut out, glued, rivetted or assembled, originate trophies, medals, award plates, indicative plates, panels, et al.
    • 本专利的特征在于扩大了用玻璃纤维增​​强的聚酯,酯类和环氧树脂的用途,将它们以普通,球形,圆柱形或其他几何形式的不可侵蚀的外观,以透明胶片,纸,布,塑料,木材制成的多色 ,金属,皮革等; 由电脑,手动或任何其他类型的打印生成。 其生产包括:在玻璃状或抛光基底上的一个或多个不饱和层; 一个或多个催化树脂层在脱模剂上; 一种或多种织造形式,织物形式或粗纱形成玻璃纤维层; 在层压板中插入透明度,纸,布,木材,金属或皮革中的多色,包含字符,图纸,绘画,图片,照片,签名等; 由电脑,手动或任何其他类型的印刷产生; 一层或多层布层; 一种或多种织造形式,织物形式或粗纱形成玻璃纤维层; 一个或多个树脂层; 应用塑料薄膜; 起泡和撤退的气泡; dismold。 层压板的多色,被切割,胶合,铆接或组装,起源于奖杯,奖牌,奖牌,指示板,面板等。