    • COLD FORMED LAMINATES
    • 冷成型层压板
    • WO2017011270A1
    • 2017-01-19
    • PCT/US2016/041365
    • 2016-07-07
    • CORNING INCORPORATED
    • FISHER, William KeithFRISKE, Mark StephenMOYER, Steven LutherRICKERL, Paul George
    • B32B17/10
    • B60J1/004B32B17/10036B32B17/10137B32B17/10761B32B17/10816B32B17/1088B32B17/10889B32B2605/006C03B23/0357
    • The principles and embodiments of the present disclosure relate generally to complexly curved laminates made from a complexly curved substrate and a flat substrate, such as automotive window glazings, and methods of cold forming complexly-curved glass products from a curved substrate and a flat substrate. In one or more embodiments, the laminate includes first complexly-curved glass substrate with a first surface and a second surface opposite the first surface, a second complexly-curved glass substrate with a third surface and a fourth surface opposite the third surface with a thickness therebetween; and a polymer interlayer affixed to the second surface and third surface, wherein the third surface and fourth surface have compressive stress values respectively that differ such that the fourth surface has as compressive stress value that is greater than the compressive stress value of the third surface.
    • 本公开的原理和实施例一般涉及由复杂弯曲的基板和诸如汽车窗玻璃的平坦基板制成的复合弯曲的层压板,以及从弯曲基板和平坦基板冷成型复杂弯曲的玻璃制品的方法。 在一个或多个实施例中,层压体包括具有第一表面和与第一表面相对的第二表面的第一复合曲面玻璃基板,具有第三表面的第二复曲面玻璃基板和与第三表面相对的第四表面, 其间; 以及固定在第二表面和第三表面上的聚合物夹层,其中第三表面和第四表面分别具有不同的压缩应力值,使得第四表面具有大于第三表面的压缩应力值的压缩应力值。
    • 10. 发明申请
    • METHODS FOR FORMING PATTERNS IN THIN GLASS LAMINATE STRUCTURES
    • 在薄玻璃层状结构中形成图案的方法
    • WO2015084902A1
    • 2015-06-11
    • PCT/US2014/068254
    • 2014-12-03
    • CORNING INCORPORATED
    • RICKERL, Paul George
    • B32B17/10C03C27/12B44F1/06
    • B32B17/10B32B17/10036B32B17/10247B32B17/10743B32B17/10761B32B17/10853B32B17/10889B32B37/06B32B37/14B32B2307/30B44C5/0407B44F1/066
    • A method of cold forming a glass laminate structure. The method includes assembling a multi-layer structure having two buffer plates and a glass laminate structure intermediate the two buffer plates, wherein one or both of the two buffer plates includes a pattern formed thereon or therein or the multi-layer structure includes non-deformable materials forming a pattern. The method further includes cold forming the glass laminate structure in the autoclave by heating the assembled structure to a temperature about 5 to 10 degrees above the softening point of the polymer interlayer for a predetermined period of time at a predetermined pressure. After processing the glass laminate structure can be removed from between the buffer plates wherein the pattern formed in or on the one or both buffer plates or non-deformable materials has been transferred to the glass laminate structure as a function of variances of thicknesses in the glass laminate structure.
    • 一种冷成型玻璃层压结构的方法。 该方法包括组装具有两个缓冲板和在两个缓冲板之间的玻璃层叠结构的多层结构,其中两个缓冲板中的一个或两个包括形成在其上或其中的图案,或者多层结构包括不可变形的 材料形成图案。 该方法还包括通过将组装结构在预定压力下将聚合物夹层的软化点加热至约5至10度的温度预定时间段,将高压釜中的玻璃层压结构冷成型。 在处理之后,可以从缓冲板之间移除玻璃层压结构,其中形成在一个或两个缓冲板上或其上的图案或不可变形材料已经作为玻璃厚度变化的函数转移到玻璃层压结构中 层压结构。