    • METHOD OF AND APPARATUS FOR MANUFACTURE OF A LAMINATE COMPRISING AN ORIENTED AND FINE-WAVED FILM, AND RESULTANT PRODUCTS
    • 包含面向薄膜和薄膜的层压板及其制品的制造方法和装置
    • WO2011006942A1
    • 2011-01-20
    • PCT/EP2010/060168
    • 2010-07-14
    • RASMUSSEN, Ole-BendtRASMUSSEN, Nikolaj
    • RASMUSSEN, Ole-BendtRASMUSSEN, Nikolaj
    • B29C55/04B29C55/18B32B3/28B32B27/06B32B27/08B32B27/10B32B27/32
    • B29C55/045B32B3/28B32B7/12B32B27/08B32B27/32B32B37/153B32B38/0012B32B2038/0028B32B2250/24B32B2307/514B32B2307/54B32B2307/5825B32B2307/704
    • In a method of manufacturing a laminate of an oriented and waved film (A) and a film or web (B), at least film (A) consisting of orientable, crystalline polymer material, the film (A) is stretched in an angular arrangement by being gripped by a linear nip (D-F) formed between rollers or bars, while being conveyed to this nip in a direction which forms an acute angle (u) to a plane perpendicular to the linear nip, and subsequently being pulled off by pulling means (1 and 2) under an acute angle (v) to the said perpendicular plane, as measured on the opposite side of this plane, (v) being greater than (u) but smaller than 85°, hereby producing elongation and uniaxial molecular orientation, the stretching ratio (GD to FE) and the angles (u) and (v) are selected such that the angle of orientation of the stretched film (A) deviates less than 15° from its longitudinal direction, and a reduction of film width is established, which measured in direct line is greater than the width reduction caused by the longitudinal elongation so as to form a longitudinally extending waving and the said waving is stabilised before meeting the pulling means (1 and 2), and film (B) is laminated to film (A) after film (A) has left the nip (D-F), while maintaining the fluting of (A). Suitably the films are formed of polyethylene.
    • 在制造取向和波浪形薄膜(A)和薄膜或网状物(B)的层压体的方法中,至少由可取向的结晶聚合物材料构成的薄膜(A),薄膜(A)以角度布置 通过在形成在辊或杆之间的线性压区(DF)夹持,同时沿着与垂直于线性压区形成锐角(u)的方向输送到该辊隙,并且随后通过拉动装置 (v)大于(u)但小于85°,这样产生的伸长率和单轴分子取向(1)和(2)与所述垂直平面成锐角(v) 选择拉伸比(GD〜FE)和角度(u)和(v),使得拉伸膜(A)的取向角从长度方向偏离小于15°,膜宽度 建立后,直线测量大于宽度减小 由纵向伸长引起的,从而形成纵向延伸的波动,并且在满足拉伸装置(1和2)之前所述波动稳定,并且膜(B)在膜(A)已经离开 (DF),同时保持(A)的凹槽。 膜适当地由聚乙烯形成。