    • ORIENTED POLYLACTIC ACID POLYMER BASED FILM
    • 取向的聚乳酸基聚合物基薄膜
    • WO2017200756A1
    • 2017-11-23
    • PCT/US2017/031043
    • 2017-05-04
    • 3M INNOVATIVE PROPERTIES COMPANY
    • MERRILL, William W.KALISH, Jeffrey P.PERCHA, Pamela A.DEHN, Derek J.GIVOT, Bradley L.KADOMA, Ignatius A.
    • C08J5/18C08L67/04B32B27/22B32B27/30B32B27/36
    • In one embodiment, a film is described comprising a mixture of semicrystalline polylactic acid polymer; polyvinyl acetate polymer having a glass transition temperature (Tg) midpoint as measured by differential scanning calorimetry of at least 25°C; and plasticizer; wherein the film is oriented. In another embodiment, a film is described comprising a mixture comprising semicrystalline polylactic acid polymer, polymer having a midpoint Tg as measured by differential scanning calorimetry of at least 25°C, and plasticizer; wherein the mixture exhibits a single midpoint Tg and the single midpoint Tg ranges from 40°C to 65°C; and wherein the film is oriented and the oriented film exhibits a higher midpoint Tg ranging from 40°C to 65°C and a lower midpoint Tg ranging from 5 to 25°C.
    • 在一个实施方案中,描述了包含半结晶聚乳酸聚合物的混合物的膜; 聚乙酸乙烯酯聚合物,其通过差示扫描量热法测量的玻璃化转变温度(Tg)中点为至少25℃; 和增塑剂; 其中薄膜是取向的。 在另一个实施方案中,描述了包含含有半结晶聚乳酸聚合物,具有通过差示扫描量热法测量的中点Tg为至少25℃的聚合物和增塑剂的混合物的膜; 其中所述混合物表现出单一中点Tg,并且所述单一中点Tg在40℃至65℃范围内; 并且其中所述薄膜被取向并且所述取向薄膜表现出在40℃至65℃范围内的较高中点Tg和在5℃至25℃范围内的较低中点Tg。