    • Yellow light afterglow material and preparation method thereof as well as LED illuminating device using same
    • 黄光余辉材料及其制备方法以及使用其的LED照明装置
    • US09045689B2
    • 2015-06-02
    • US13497129
    • 2009-11-09
    • Hongjie ZhangMing ZhangChengyu LiKun ZhaoHao Zhang
    • Hongjie ZhangMing ZhangChengyu LiKun ZhaoHao Zhang
    • C09K11/80H01L33/00C09K11/77H01L33/50
    • C09K11/7774H01L25/0753H01L33/502
    • The invention relates to a yellow light afterglow material and a preparation method thereof as well as an LED illuminating device using the same. The yellow light afterglow material comprises the chemical formula of aY2O3.bAl2O3.cSiO2:mCe.nB.xNa.yP, where a, b, c, m, n, x and y are coefficients, and a is not less than 1 but not more than 2, b is not less than 2 but not more than 3, c is not less than 0.001 but not more than 1, m is not less than 0.0001 but not more than 0.6, n is not less than 0.0001 but not more than 0.5, x is not less than 0.0001 but not more than 0.2, and y is not less than 0.0001 but not more than 0.5; wherein Y, Al and Si are substrate elements, and Ce, B, Na and P are activators. The yellow light afterglow material is prepared by the following steps: weighing oxides of elements or materials which can generate oxides at high temperature by molar ratio as raw materials, evenly mixing and then sintering the raw materials at 1200-1700° in a reducing atmosphere.
    • 本发明涉及一种黄光余辉材料及其制备方法以及使用其的LED照明装置。 黄光余辉材料包括aY2O3.bAl2O3.cSiO2:mCe.nB.xNa.yP的化学式:其中a,b,c,m,n,x和y是系数,a不小于1但不是 大于2,b不小于2,但不大于3,c不小于0.001,但不大于1,m不小于0.0001,但不大于0.6,n不小于0.0001,但不大于 0.5,x不小于0.0001但不大于0.2,y不小于0.0001但不大于0.5; 其中Y,Al和Si是底物,Ce,B,Na和P是活化剂。 黄光余辉材料通过以下步骤制备:将以高摩尔比生成氧化物的元素或材料的氧化物称重为原料,均匀混合,然后在还原气氛中在1200-1700℃下烧结原料。