    • 10. 发明授权
    • Method for producing granular composition
    • 生产粒状组合物的方法
    • US08187510B2
    • 2012-05-29
    • US12662122
    • 2010-03-31
    • Hideaki AwaMasato AraiHajime Shinomiya
    • Hideaki AwaMasato AraiHajime Shinomiya
    • B29B9/08
    • C08K5/1345B29B9/02C08K5/005C08K5/372Y02P20/582
    • A method for producing a granular composition including the steps of: stirring and granulating a mixture containing not less than 3 parts by weight and not more than 80 parts by weight of a phenol compound represented by the formula (1): wherein R1 is an alkyl group having 1 to 8 carbon atoms, X is an n-valent alcohol residue having 1 to 18 carbon atoms optionally containing a heteroatom, a cyclic group, or a heteroatom and a cyclic group, and n is an integer of 1 to 4, and not less than 20 parts by weight and not more than 50 parts by weight of a binder to obtain a granular agglomerate; and cracking the granular agglomerate at a temperature equal to or lower than the melting point of the binder and equal to or higher than the temperature which is 10° C. lower than the melting point, through a cracking machine equipped with a separation mechanism capable of recovering a granule having a particle size of not more than 5 mm, and a cracking mechanism, to obtain a granule.
    • 一种颗粒状组合物的制造方法,其特征在于,包括以下步骤:将含有不少于3重量份且不超过80重量份由式(1)表示的酚化合物的混合物进行搅拌和造粒:其中R1是烷基 具有1至8个碳原子的基团,X是任选含有杂原子,环状基团或杂原子和环状基团的具有1至18个碳原子的n价醇残基,n是1至4的整数,并且 不少于20重量份且不超过50重量份的粘合剂,以获得颗粒聚集体; 在等于或低于粘合剂熔点的温度下,通过配备有分离机构的裂解装置将熔融点熔点等于或高于熔点低10℃的温度下破碎, 回收粒径不大于5mm的颗粒和破裂机理,得到颗粒。