    • 4. 发明授权
    • Process for phosphatizing metals
    • 磷化金属的工艺
    • US4419199A
    • 1983-12-06
    • US373475
    • 1982-04-30
    • Dieter HauffeGerhard MullerWerner RauschGudrun Volling
    • Dieter HauffeGerhard MullerWerner RauschGudrun Volling
    • C23C22/12C23C22/13C23C22/36C23C22/77C23F7/10C23F7/12C25D13/06C25D13/20
    • C23C22/362C23C22/12
    • A process for the phosphatizing of metals, particularly iron, steel and zinc, in which the metal is contacted with acidic aqueous zinc phosphate solutions, containing an oxidizing agent, which containfrom 0.4 to 1.5 g/liter of Zn,from 0 to 1.3 g/liter of Ni andfrom 10 to 26 g/liter of P.sub.2 O.sub.5,and in which the weight ratio of Zn to P.sub.2 O.sub.5 is adjusted to a value of (from 0.012 to 0.12):1 and of Ni to Zn to a value of (from 0 to 1.5):1, and the bath is supplemented with a concentrate, in which Zn, Ni and P.sub.2 O.sub.5 are present in a weight ratio of (from 0.18 to 0.33:(from 0 to 0.06):1, so as to obtain satisfactory phosphatizing results over a long period.Preferably, the zinc phosphatizing solutions, which, in addition, may also contain simple or complex fluorides and compounds that reduce the weight of the coat, are applied at a temperature within the range of from 30.degree. to 65.degree. C.
    • 一种金属,特别是铁,钢和锌的磷酸化方法,其中金属与酸性磷酸锌水溶液接触,含有氧化剂,其含有0.4-1.5g /升Zn,0-3.3g /升的Ni和10〜26g /升的P 2 O 5,并且其中将Zn与P 2 O 5的重量比调节至(0.012至0.12):1,Ni至Zn的值(从 0至1.5):1,浴中补充有以重量比(0.18-0.33:(0-0.06):1)存在的Zn,Ni和P 2 O 5的浓缩物,以获得令人满意的 优选地,磷酸锌溶液还可以含有简单或复合的氟化物和降低涂层重量的化合物,其温度范围为30°至65° DEG C.
    • 5. 发明授权
    • Method of providing an anti-stick coating on non-oriented,
semi-processed electrical steels to be subjected to a quality anneal
    • 在未取向的半加工电工钢上提供防粘涂层以进行质量退火的方法
    • US4367101A
    • 1983-01-04
    • US251136
    • 1981-04-06
    • Michael H. HaselkornJames D. Evans
    • Michael H. HaselkornJames D. Evans
    • C23C22/00C21D1/70C21D9/46C23C22/08C23C22/20C23C22/74H01F1/147C23F7/10
    • H01F1/14783C21D1/70C23C22/74
    • A process of providing an inorganic anti-stick coating directly on non-oriented, semi-processed electrical steels by applying to such steels a coating solution containing Al.sup.+++, Mg.sup.++, and H.sub.2 PO.sub.4.sup.- in a specified relative relationship, the concentration of Al.sup.+++, Mg.sup.++, and H.sub.2 PO.sub.4.sup.- comprising 100 parts by weight calculated as Al.sub.2 O.sub.3, MgO and H.sub.3 PO.sub.4, respectively, on a water-free basis. The coating solution may additionally contain from 0 to 150 parts by weight of colloidal silica on a water-free basis. Chromic anhydride (C.sub.r O.sub.3) may be added to the coating solution to improve its wettability and improve the moisture resistance of the anti-stick coating. The coating solution is so diluted with water as to provide a uniform coating as thin as possible to prevent lamination sticking and having a coating weight of less than 2 grams per square meter on each side. The coated electrical steel is subjected to a heat treatment to cure the anti-stick coating thereon.
    • 通过向这种钢施加含有Al +++,Mg ++和H 2 PO 4 - 的涂层溶液,以特定的相对关系,直接在无取向的半加工电工钢上提供无机防粘涂层,Al +++,Mg ++, 和H 2 PO 4 - 分别包含100重量份,以无水基计算为Al 2 O 3,MgO和H 3 PO 4。 涂布溶液可以在无水基础上另外含有0至150重量份的胶体二氧化硅。 可以向涂料溶液中加入铬酸酐(CrO 3)以改善其润湿性并提高防粘涂层的耐湿性。 涂覆溶液用水稀释,以提供尽可能薄的均匀涂层,以防止层压粘结,并且每侧具有小于2克/平方米的涂层重量。 对涂覆的电工钢进行热处理以固化其上的防粘涂层。