    • 3. 发明申请
    • Hot-rolled steel wire and rod for machine structural use and a method for production the same
    • 用于机器结构用途的热轧钢丝和棒材及其制造方法
    • US20030015264A1
    • 2003-01-23
    • US09829742
    • 2001-07-06
    • Hideo KanisawaTatsuro OchiManabu KubotaKoji TanabeKiichiro Tsuchida
    • C21D007/13
    • C21D8/06C21D7/13C21D9/5732C21D2211/003C21D2211/005
    • The present invention provides a hot rolled steel wire rod or bar for machine structural use having, in the as-hot-rolled condition, cold workability equal to that of the conventional wire rods or bars softened through annealing after hot rolling, and a method to produce the same: and relates to a hot rolled steel wire rod or bar for machine structural use, characterized in that; the wire rod or bar is made from a steel consisting of, in weight, 0.1 to 0.5% of C, 0.01 to 0.5% of Si, 0.3 to 1.5% of Mn, and the balance comprising Fe and unavoidable impurities and containing strengthening elements as required; its microstructure consists of ferrite and pearlite; its ferrite crystal grain size number defined under Japanese Industrial Standard (JIS) G 0552 is 11 or higher; and a granular carbide 2 nullm or less in circle-equivalent diameter and having an aspect ratio of 3 or less accounts for a percentage area of 3 to 15%.
    • 本发明提供一种用于机械结构用途的热轧钢线材或棒材,其在热轧条件下具有与通过热轧后退火软化的常规线材或棒材相当的冷加工性能,以及 制造相同的材料:涉及用于机械结构用途的热轧钢线材或棒材,其特征在于: 线材或棒材由重量为0.1〜0.5%的C,0.01〜0.5%的Si,0.3〜1.5%的Mn,余量由Fe和不可避免的杂质构成的钢制成,含有强化元素为 需要; 其微结构由铁素体和珠光体组成; 日本工业标准(JIS)G 0552规定的铁素体晶粒尺寸数为11以上; 圆周当量直径为2μm以下,长径比为3以下的粒状碳化物占3〜15%的面积的比例。
    • 4. 发明申请
    • Method of manufacturing fe-ni alloy
    • 制造合金的方法
    • US20020043314A1
    • 2002-04-18
    • US09942482
    • 2001-08-30
    • Nippon Mining & Metals Co. , Ltd.
    • Masatoshi Eto
    • C21D007/13
    • C21D8/0205B21B1/26B21B3/02C21D8/0226
    • A method of manufacturing an improved FenullNi alloy consisting of 33-37% Ni; 0.001-0.1% Mn; optionally, 0.01-2% Co; and at least one of (1) 0.01-0.8% Nb; (2) 0.01-0.8% Ta; and/or (3) 0.01-0.8% Hf, with the total of Nb, Ta and Hf being in the range of 0.01-0.8% and the remainder being Fe and unavoidable impurities. The method comprises subjecting the alloy to a hot rolling process wherein the rate of distortion during each pass of hot rolling is below 70/second resulting in the alloy having a reduced rate of crack formation during the hot rolling process, and high drop-shock resistance and low thermal expansion after the hot rolling process.
    • 一种由33-37%Ni构成的改进的Fe-Ni合金的制造方法; 0.001-0.1%Mn; 任选地,0.01-2%Co; 和(1)0.01-0.8%Nb中的至少一种; (2)0.01-0.8%Ta; 和/或(3)0.01-0.8%Hf,其中Nb,Ta和Hf的总量在0.01-0.8%的范围内,余量为Fe和不可避免的杂质。 该方法包括对合金进行热轧过程,其中每次热轧过程中的变形率低于70 /秒,导致合金在热轧过程中裂纹形成速率降低,并且具有高的耐跌落冲击性 热轧后的热膨胀率低。