    • Process for producing biodegradable molded item and molding dies therefor
    • 用于制造生物可降解模塑制品的方法和模具
    • US08043539B2
    • 2011-10-25
    • US10507507
    • 2003-03-12
    • Akio OzasaAkihisa HashimotoRumi ShinoharaShinji TanakaTakeshi Shingu
    • Akio OzasaAkihisa HashimotoRumi ShinoharaShinji TanakaTakeshi Shingu
    • B29C44/06B32B9/00
    • B29C43/184B29C33/10B29C43/003B29C43/206B29C43/36B29C44/14B29C44/3426B29C44/569B29K2105/04B29K2995/0059B29L2031/712
    • Using a metal mold (20a) consisting of a convex mold part (21a) and a concave mold part (22a), a molding material (14) is placed between a pair of coating films (12), and after clamping, the molding material (14) and the coating film (12) are heated and molded to make a biodegradable expanded molded article, and at the same time, the coating film (12) is softened and pressure-bonded to a surface of the biodegradable expanded molded article. An exhaust hole (31a) and (32a) are provided on the convex mold part (21a) and the concave mold part (22a), respectively. At the time of heating and molding, gaseous matter existing between the coating film (12) and a surface of the metal mold (20a) is discharged out of the metal mold (20a) through the exhaust holes (31a) and (32a). Accordingly, it is possible to provide a method and a mold to manufacture a biodegradable expanded molded article easily and with excellent accuracy of dimension, having enough strength, enough water resistance, very excellent biodegradability and excellent surface smoothness even if the biodegradable molded article has a complicated shape.
    • 使用由凸模部件(21a)和凹模部件(22a)组成的金属模具(20a),将成型材料(14)放置在一对涂膜(12)之间,并且在夹紧之后,模制材料 (14)和涂膜(12)进行加热成型,制成生物降解性发泡成形体,同时将涂膜(12)软化并压接在生物降解性发泡成形体的表面。 排气孔(31a)和(32a)分别设置在凸模部分(21a)和凹模部分(22a)上。 在加热和模塑时,存在于涂膜(12)和金属模具(20a)的表面之间的气体通过排气孔(31a)和(32a)从金属模具(20a)排出。 因此,即使可生物降解的成型体具有可以生物降解的成型体,也可以容易且具有优异的尺寸精度,具有足够的强度,足够的耐水性,极好的生物降解性和优异的表面平滑性来制造可生物降解的发泡成型体的方法和模具 复杂的形状。
    • 3. 发明授权
    • Method of recycling waste plastic foam materials
    • 回收废塑料泡沫材料的方法
    • US07943676B2
    • 2011-05-17
    • US12027517
    • 2008-02-07
    • Kun-Huang Chang
    • Kun-Huang Chang
    • C08J11/04
    • B29B17/0026B29B17/0404B29B17/0412B29C44/12B29C44/3426B29C44/3442B29K2075/00B29K2105/04C08G18/7621C08G2101/0083C08J9/0061C08J9/35C08J2375/04C08J2475/00Y02P20/582Y02W30/62Y02W30/625
    • A method of recycling waste plastic foam materials firstly is to smash a waste material including polyurethane foam into fine particles so as to obtain a first starting material. The first starting material is then crisped and followingly milled into powder so as to obtain a second starting material. The second starting material is then placed into a mixer to mix with a first foaming reaction solution including polyol, catalyst and additives injected into the mixer so as to form a semi-treated foaming material. And then, the semi-treated foaming material is mixed with a second foaming reaction solution including diisocyanate injected into the mixer so as to obtain a completed-treated foaming material. Lastly, the completed-treated foaming material is poured into a mold and then water vapor is uniformly introduced into the mold so as to induce the completed-treated foaming material to proceed foaming reaction.
    • 首先回收废塑料泡沫材料的方法是将包括聚氨酯泡沫的废料粉碎成细颗粒,以获得第一起始材料。 然后将第一起始材料脆化并随后研磨成粉末,以获得第二起始原料。 然后将第二起始原料放入混合器中以与注入混合器中的多元醇,催化剂和添加剂的第一发泡反应溶液混合以形成半处理的发泡材料。 然后,将半处理的发泡材料与包含二异氰酸酯的第二发泡反应溶液混合到混合器中,以获得经完成处理的发泡材料。 最后,将完成处理的发泡材料倒入模具中,然后将水蒸汽均匀地引入模具中,以引起经完成处理的发泡材料进行发泡反应。
    • 4. 发明申请
    • PROCESS AND DEVICE FOR PRODUCING BLOCKS OF MATERIAL
    • 用于生产材料块的方法和装置
    • US20100092597A1
    • 2010-04-15
    • US12530097
    • 2008-02-28
    • Angelo Candiracci
    • Angelo Candiracci
    • B29C44/28
    • B29C44/26B29C44/206B29C44/3426B29C44/445B29C44/58
    • In a process and a device for producing blocks of expanded polystyrene, a loose mass (7) of polystyrene spheres is expanded in a mould (2-3), where a rear surface (9) of the polystyrene block (8) previously produced delimits the mould forming chamber. Therefore, through adherence the newly formed block (7-8) is joined to the rear end (9) of the block previously formed, and the block (8) made in this way is fed forward until it forms the rear end (9) for another newly expanded block (8), and so on to produce a sort of continuous block (8), which can be formed for cutting to any desired size, without producing any waste.
    • 在用于制造发泡聚苯乙烯块的方法和装置中,将松散的聚苯乙烯球体(7)在模具(2-3)中膨胀,其中先前产生的聚苯乙烯块(8)的后表面(9)界定 模具成型室。 因此,通过粘合,将新形成的块体(7-8)接合到预先形成的块体的后端部(9),并且以这种方式制成的块体(8)向前馈送,直到形成后端部(9) 对于另一个新膨胀的块(8),等等以产生可以形成为切割成任何所需尺寸的一种连续块(8),而不产生任何浪费。
    • 7. 发明申请
    • Foam molding die apparatus
    • 泡沫成型模具设备
    • US20010021402A1
    • 2001-09-13
    • US09790728
    • 2001-02-23
    • Iwao NoharaShigeki YoshimuraKiyotaka Ida
    • B29C045/20
    • B29C44/3426B29C44/1233B29C44/588
    • A foam molding die apparatus integrally molds a top side member and a back side member via a foam member. This apparatus comprises a plurality of work piece nozzles. Of these nozzles, the nozzles for supplying heating steam is structured so that a cylindrical body of which a work piece flow passage having a vent hole incapable of passing raw material beads is formed at a tip end portion is mounted to a die via a heat buffering member. In addition, the above nozzles may be structured so that means for forming a vent hole incapable of passing raw material beads is disposed in a synthetic resin based pipe forming a work piece flow passage. The work piece nozzles are preferably disposed with intervals of at least 100 mm on the outer face of a die at a portion at which the thickness of a foam molder is less than 10 mm. With respect to a portion at which the thickness of the foam molder is 10 mm or more, these nozzles are preferably disposed with intervals of at least 150 mm.
    • 泡沫成型模具设备通过泡沫构件一体地模制顶侧构件和后侧构件。 该装置包括多个工件喷嘴。 在这些喷嘴中,用于提供加热蒸汽的喷嘴被构造成使得在顶端部分处形成具有不能通过原料珠的通气孔的工件流动通道的圆筒体通过热缓冲 会员。 此外,上述喷嘴可以构造成使得形成不能通过原料珠的通气孔的装置设置在形成工件流动通道的合成树脂基管中。 在泡沫成型机的厚度小于10mm的部分,工件喷嘴优选地在模具的外表面上以至少100mm的间隔设置。 关于泡沫成型机的厚度为10mm以上的部分,这些喷嘴优选以至少150mm的间隔设置。