    • 8. 发明授权
    • Process for producing carbon fibers
    • 生产碳纤维的方法
    • US4069297A
    • 1978-01-17
    • US674244
    • 1976-04-06
    • Kazuhisa SaitoHiroyasu Ogawa
    • Kazuhisa SaitoHiroyasu Ogawa
    • D01F9/14D01F9/22D01F9/32D01F9/12
    • D01F9/14D01F9/22D01F9/32
    • A process for continuously producing carbon fibers which comprises preoxidizing polyacrylonitrile fibers containing at least about 90% by weight of acrylonitrile at a temperature of about 200.degree. to about 300.degree. C in an oxidizing atmosphere while allowing the fibers to shrink about 40 to about 70% (of the free shrinkage of the fibers determined under a load of 1 mg/d) with the progress of preoxidation; then carbonizing the preoxidized fibers at about 500.degree. to about 1,000.degree. C in a non-oxidizing atmosphere so that the shrinkage of the fibers finally becomes about 40 to about 70% (of the free shrinkage of the preoxidized fibers determined when the fibers are placed under a load of 1 mg/d and heated at 1,000.degree. C for 15 minutes); and then heat treating the carbonized fibers at constant length at a temperature of up to about 3,000.degree. C in a non-oxidizing atmosphere.
    • 一种连续生产碳纤维的方法,其包括在约200至约300℃的温度下在氧化气氛中预氧化含有至少约90重量%的丙烯腈的聚丙烯腈纤维,同时使纤维收缩约40至约70% (在1mg / d的负荷下测定的纤维的自由收缩)随着预氧化的进行; 然后在非氧化气氛中将约500℃至约1000℃的预氧化纤维碳化,使得纤维的收缩最终变为约40至约70%(当放置纤维时测定的预氧化纤维的自由收缩率 在1mg / d的负荷下,在1000℃下加热15分钟); 然后在非氧化性气氛中在高达约3000℃的温度下以恒定长度热处理碳化纤维。
    • 9. 发明授权
    • Apparatus for continuous production of carbon fibers
    • 用于连续生产碳纤维的设备
    • US4753777A
    • 1988-06-28
    • US743843
    • 1985-06-12
    • Osamu YoshinariMakoto SugiyamaHideki Nakai
    • Osamu YoshinariMakoto SugiyamaHideki Nakai
    • D01F9/14D01F9/16D01F9/22D01F9/32F27D11/02B01J15/00
    • D01F9/22D01F9/14D01F9/16D01F9/32F27D11/02
    • A method for producing carbon fibers in a vertical carbonizing furnace and an apparatus for producing carbon fibers using such a method are disclosed. The furnace includes a heating chamber for carbonizing fibers, the furnace including,(i) a fiber inlet at the upper end of the chamber(ii) an air tight sealed fiber outlet at the lower end of the furnace,(iii) an inert gas inlet provided on the wall of the chamber and above the fiber outlet,(iv) at least one inert gas injection portion, formed on the wall of the chamber, each capable of forming a curtain of inert gas across the heating chamber, each injection portion being provided between the gas inlet and the fiber inlet,(v) at least one outlet each being provided below each inert gas injection portion, and(vi) a heating member capable of controlling the temperature in the heating chamber in such a manner that the temperature gradually increases from the upper end toward a lower end of the heating chamber. The carbon fibers produced by this method or apparatus are excellent in that they have few fluffs and cohering filaments and improved strength and ductility.
    • 公开了一种在立式碳化炉中生产碳纤维的方法和使用这种方法生产碳纤维的设备。 该炉包括用于碳化纤维的加热室,炉包括:(i)在炉的上端的纤维入口(ii)在炉下端的气密密封的纤维出口,(iii)惰性气体 入口设置在腔室的壁上并在纤维出口的上方,(iv)至少一个惰性气体注入部分,形成在腔室的壁上,每个惰性气体注入部分能够跨越加热室形成惰性气体帘幕,每个注射部分 设置在气体入口和纤维入口之间,(v)至少一个出口,每个出口设置在每个惰性气体注入部分的下方,以及(vi)加热构件,其能够以这样的方式控制加热室中的温度: 温度从加热室的上端向下端逐渐增加。 通过该方法或装置制造的碳纤维的优点是它们具有很少的绒毛和绒毛长丝,并且具有改善的强度和延展性。