    • 1. 发明授权
    • Method of conditioning foam materials by compression
    • 通过压缩调节泡沫材料的方法
    • US06495085B1
    • 2002-12-17
    • US09627464
    • 2000-07-28
    • Clay SimpsonRick D. Lawson
    • Clay SimpsonRick D. Lawson
    • B29C6720
    • B29C44/5627B29C43/003B29K2079/08B29K2105/04B29K2995/0002
    • The inventive method comprises compressing roughly half a bun of polyimide foam at a rate of no more than 12 feet per minute from its initial height of approximately 15″, until it reaches a compressed height of no more than 2″. The compression is maintained on the bun for no more than one minute, and then released. The half-bun is then permitted to expand, and it will rebound to approximately 90-95% of its initial height. This conditioned foam may then be cut or otherwise formed into acoustical panels of varying heights and/or configurations, without worry about the ultimate shrinkage after treatment. In addition the treated half-bun may be cut into irregular shapes of more varying dimensions, up to the maximum dimension of the treated half-bun.
    • 本发明的方法包括从大约15“的初始高度以不超过12英尺每分钟的速度压缩大约一半的聚酰亚胺泡沫,直到其达到不超过2”的压缩高度。 压缩保持在馒头上不超过一分钟,然后释放。 半is然后被允许扩张,并将反弹到初始高度的大约90-95%。 然后可以将经调理的泡沫切割或以其它方式形成为不同高度和/或构型的声学板,而不用担心处理后的最终收缩。 此外,经处理的半馒头可以被切割成更多变化的尺寸的不规则形状,直到被处理的半the的最大尺寸。