    • 3. 发明授权
    • Glasses and glass-ceramics with high specific young's modulus and their applications
    • 玻璃和玻璃陶瓷具有较高的特定年龄模量及其应用
    • US06376402B1
    • 2002-04-23
    • US09551993
    • 2000-04-19
    • Wolfgang PannhorstUte WoelfelSilke Wolff
    • Wolfgang PannhorstUte WoelfelSilke Wolff
    • C03L3091
    • C03C3/064C03C3/091C03C10/0027
    • The glass or glass-ceramic has the following composition (in % by weight based on oxide content): SiO2, 25 to 50; B2O3, >5 to 16; Al2O3, 10 to 17; P2O5, 0 to 8; Li2O,5 to 15; Na2O, 0 to 10; K2O, 0 to 10; MgO, 10 to 30; CaO, 0 to 10; SrO, 0 to 8; ZnO, 0 to 8; TiO2, 0.1 to 10; ZrO2, 0 to 8; and at least one refining agent, in an amount as needed according to its purpose. The sum total amount of divalent metal oxides (RO) present is less or equal to than 45% by weight based on oxide content and the sum total amount of alkali metal oxides (R2O) present is less than or equal to 30% by weight based on oxide content. The glass or glass-ceramic material generally has elasticity modulus values (E)>90×103 N/mm2 and 30×105 N cm/g and 7.0×10−6/K and
    • 玻璃或玻璃陶瓷具有以下组成(以氧化物含量为基准的重量%):SiO 2,25〜50; B2O3,> 5〜16; Al2O3,10〜17; P2O5,0至8; Li2O,5〜15; Na2O,0〜10; K2O,0〜10; MgO,10〜30; CaO,0〜10; SrO,0〜8; ZnO,0〜8; TiO2,0.1〜10; 0〜8; 和至少一种澄清剂,其量根据其目的需要。 存在的二价金属氧化物(RO)的总量相对于氧化物含量小于或等于45重量%,碱存在的碱金属氧化物(R2O)的总量相对于基于 对氧化物含量。 玻璃或玻璃 - 陶瓷材料的弹性模量值(E)通常具有> 90×10 3 N / mm 2和<125×10 3 N / mm 2的弹性模量值,比弹性模量值(E / rho)> 30×105Ncm / g和<45×105Ncm / g, 热膨胀系数值(α20/ 300)> 7.0×10-6 / K和<11.0×10-6 / K。 该材料非常适合制作固定盘基片。
    • 5. 发明授权
    • Method for the manufacture of dense-sintered glass ceramic moldings
    • 致密烧结玻璃陶瓷模制品的制造方法
    • US5922271A
    • 1999-07-13
    • US868578
    • 1997-06-04
    • Wolfgang SemarJanusz ZborowskiWolfgang PannhorstWaldemar WeinbergKlaus MirschMichael DunklBartolome AloyWerner WaidhasMonika Burkner
    • Wolfgang SemarJanusz ZborowskiWolfgang PannhorstWaldemar WeinbergKlaus MirschMichael DunklBartolome AloyWerner WaidhasMonika Burkner
    • C03B19/06C03C3/083C03C10/00C03C10/12B28B1/26
    • C03C10/0027
    • A method for the manufacture of dense-sintered glass-ceramic shaped objects which have a coefficient of thermal expansion, .alpha., of -0.5.times.10.sup.-6 /K to 1.8.times.10.sup.-6 /K in the range between 20.degree. C. and 700.degree. C. whereby ceramizable glass powder and/or glass-ceramic powder from the system Li.sub.2 O-Al.sub.2 O.sub.3 -SiO.sub.2 is slip-cast by means of porous molds, dried, pretempered if necessary at temperatures up to 600.degree. C., vitrified and then sintered until the sintering temperature is reached up to relative densities of greater than 0.96 and ceramized, and whereby the glass powder and/or the glass ceramic-powder is prepared in a first grain size fraction of less than 63 .mu.m, in particular less than 45 .mu.m, and in a second grain size fraction of less than 7 .mu.m, in a ratio of the fractions to one another between 2:1 and 4:1, to form a stable, pourable slurry. The method can be used for the manufacture of industrial ceramics, but also for the manufacture of complex-shaped, large-volume and thin-walled hollow containers, in particular for use as cooking utensils which are resistant to thermal shock, as well as for dinnerware, solid ceramic castings and composites.
    • 一种在20℃至700℃的范围内制造具有-0.5×10 -6 / K至1.8×10 -6 / K的热膨胀系数α的致密烧结玻璃 - 陶瓷成型物体的方法 C.由系统Li2O-Al2O3-SiO2的可陶瓷化玻璃粉末和/或玻璃陶瓷粉末通过多孔模具进行滑移浇铸,干燥,如果需要,在高达600℃的温度下进行预硫化,玻璃化,然后烧结直到 烧结温度达到大于0.96的相对密度并陶瓷化,由此玻璃粉末和/或玻璃陶瓷粉末以小于63μm,特别是小于45μm的第一粒度级分制备 m,并且在小于7μm的第二粒度分数中,以2:1和4:1之间的馏分之间的比例,形成稳定的可倾倒浆料。 该方法可用于工业陶瓷的制造,也可用于制造复杂形状的大容量和薄壁中空容器,特别是用作耐热冲击的炊具,以及用于 餐具,固体陶瓷铸件和复合材料。