    • Information recording medium and process for producing the same
    • 信息记录介质及其制造方法
    • US07524612B2
    • 2009-04-28
    • US10516244
    • 2003-05-23
    • Yasuo HosodaAyumi MitsumoriMegumi SatoMasataka YamaguchiTomoaki IzumiSatoshi JinnoYoichi Okumura
    • Yasuo HosodaAyumi MitsumoriMegumi SatoMasataka YamaguchiTomoaki IzumiSatoshi JinnoYoichi Okumura
    • G11B7/24
    • G11B7/266G11B7/243G11B2007/24306G11B2007/24312G11B2007/24314G11B2007/24322Y10S430/146
    • An information recording medium has an excellent jitter characteristic with a considerable difference in reflectance between prior to and subsequent to recording. The information recording medium includes a recording layer which contains a material having a reflectance which varies by irradiation of a light beam, on which information is recorded as reflectance variations, and a substrate for supporting the recording layer, the recording layer including a metal nitride as a major component. In a method of manufacturing the information recording medium having a recording layer which includes a material having a reflectance which varies by irradiation of a light beam, on which information is recorded as reflectance variations, and the substrate for supporting the recording layer, the recording layer including a metal nitride as a major component, the method includes a recording layer forming step for forming the recording layer by a reactive sputtering method which uses a target comprised of a metal constituting a metal nitride, wherein a flow ratio Ar:N2 in an atmosphere including Ar and N2 in the recording layer forming step is set within the range of 80:10 to 10:80.
    • 信息记录介质具有优异的抖动特性,在记录之前和之后具有相当大的反射率差异。 该信息记录介质包括一记录层,该记录层含有具有反射率的材料,其反射率随着光束的照射而变化,信息被记录为反射率变化,以及用于支撑该记录层的基板,该记录层包括一金属氮化物 一个主要组成部分。 在制造具有记录层的信息记录介质的方法中,记录层包括具有通过照射光束而变化的反射率的材料,其上记录信息作为反射率变化,以及用于支撑记录层的基板,记录层 包括金属氮化物作为主要成分的方法,所述方法包括用反应溅射法形成记录层的记录层形成步骤,所述反应溅射法使用由构成金属氮化物的金属组成的靶,其中气氛中的流量比Ar:N 2 包括记录层形成步骤中的Ar和N 2设定在80:10至10:80的范围内。