    • A process for the production of a honeycomb-like porous body of 10 to 1000 nm in thickness which is made of a water-insoluble polymer and has pores having diameters of 10 to 100 nm, which comprises the following steps: (1) the step of dissolving a water-insoluble polymer in a water-incompatible organic solvent having a surface tension (γL) of 50 dyne/cm or below to prepare a solution of the polymer in the organic solvent, (2) the step of applying the solution prepared in the step (1) to the surface of a substrate with the proviso that the surface tension (γS) of the substrate, the surface tension (γL) of the organic solvent, and the surface tension (γSL) between the substrate and the solvent satisfy the relationship: γS−γSL>γL, and (3) the step of bringing the solution applied on the substrate into contact with air having a relative humidity of 30% or above to evaporate the organic solvent at such a rate that the coating thickness at applying the solution to the surface of the substrate is reduced to one-fifth within one second.
    • 一种制造厚度为10〜1000nm的蜂窝状多孔体的方法,该蜂窝状多孔体由水不溶性聚合物制成,具有直径为10〜100nm的孔,其包括以下步骤:(1)步骤 将水不溶性聚合物溶解在表面张力(γL)为50达因/厘米或更低的水不相容的有机溶剂中以制备聚合物在有机溶剂中的溶液,(2)将制备的溶液 在步骤(1)中到基底的表面,条件是基材的表面张力(γS),有机溶剂的表面张力(γL)和基材和溶剂之间的表面张力(γSL) 满足γS-γSL>γL的关系,(3)将施加在基板上的溶液与相对湿度为30%以上的空气接触的步骤,以使涂布厚度 在应用解决方案 衬底的表面在一秒钟内减少到五分之一。
    • 5. 发明申请
    • Process For Production Of Submicrohoneycomb Structures
    • 亚微米结构的生产工艺
    • US20080032048A1
    • 2008-02-07
    • US11661620
    • 2005-08-25
    • Masatsugu ShimomuraHiroshi Yabu
    • Masatsugu ShimomuraHiroshi Yabu
    • C08J9/28B29C41/12B29C41/24C08L101/00B29L7/00B82B3/00
    • B29C41/28B29C41/12B29C48/11B29D24/005B29D99/0089B29L2031/60B29L2031/756C08J9/28C08J2201/0502
    • A process for the production of a honeycomb-like porous body of 10 to 1000 nm in thickness which is made of a water-insoluble polymer and has pores having diameters of 10 to 100 nm, which comprises the following steps: (1) the step of dissolving a water-insoluble polymer in a water-incompatible organic solvent having a surface tension (γL) of 50 dyne/cm or below to prepare a solution of the polymer in the organic solvent, (2) the step of applying the solution prepared in the step (1) to the surface of a substrate with the proviso that the surface tension (γS) of the substrate, the surface tension (γL) of the organic solvent, and the surface tension (γSL) between the substrate and the solvent satisfy the relationship: γS−γSL>γL, and (3) the step of bringing the solution applied on the substrate into contact with air having a relative humidity of 30% or above to evaporate the organic solvent at such a rate that the coating thickness at applying the solution to the surface of the substrate is reduced to one-fifth within one second.
    • 一种制造厚度为10〜1000nm的蜂窝状多孔体的方法,该蜂窝状多孔体由水不溶性聚合物制成,具有直径为10〜100nm的孔,其包括以下步骤:(1)步骤 将水不溶性聚合物溶解在表面张力(γL)为50达因/厘米或更低的水不相容的有机溶剂中以制备聚合物在有机溶剂中的溶液,(2)将制备的溶液 在步骤(1)中到基底的表面,条件是基材的表面张力(γS),有机溶剂的表面张力(γL)和基材和溶剂之间的表面张力(γSL) 满足γS-γSL>γL的关系,(3)将施加在基板上的溶液与相对湿度为30%以上的空气接触的步骤,以使涂布厚度 在应用解决方案 衬底的表面在一秒钟内减少到五分之一。