    • 2. 发明授权
    • Processes for making aerogel-electrolyte-metal composites
    • 制备气凝胶 - 电解质 - 金属复合材料的方法
    • US07247259B2
    • 2007-07-24
    • US11098095
    • 2005-04-04
    • Can ErkeyHiroaki S. Hara
    • Can ErkeyHiroaki S. Hara
    • H01B1/02H01B1/04B05D5/00B05D3/02B05D7/00
    • H01M4/92B01J13/0091H01M4/8605H01M4/885H01M2008/1095
    • A process for making an aerogel-electrolyte-metal composite includes contacting an aerogel with an electrolyte to form an aerogel-electrolyte composite; contacting the aerogel-electrolyte composite with a metal precursor to form an aerogel-electrolyte-precursor composite; and converting the metal precursor of the aerogel-electrolyte-precursor composite to metal crystals to form the aerogel-electrolyte-metal composite. In addition, an aerogel-electrolyte-metal composite is formed by the process, wherein the average longest dimension of the metal crystals is about 1 to about 3 nanometers, and wherein the metal crystals are about 30% to about 100% dispersed.
    • 制备气凝胶 - 电解质 - 金属复合材料的方法包括使气凝胶与电解质接触以形成气凝胶 - 电解质复合材料; 使气凝胶 - 电解质复合材料与金属前体接触以形成气凝胶 - 电解质 - 前体复合材料; 并将气凝胶 - 电解质 - 前体复合材料的金属前体转化为金属晶体以形成气凝胶 - 电解质 - 金属复合材料。 此外,通过该方法形成气凝胶 - 电解质 - 金属复合材料,其中金属晶体的平均最长尺寸为约1至约3纳米,并且其中金属晶体为约30%至约100%分散。