    • Battery having replaceable electrodes
    • 电池具有可更换电极
    • US4421830A
    • 1983-12-20
    • US384914
    • 1982-06-04
    • Richard T. SchneiderFrederick A. Hauck
    • Richard T. SchneiderFrederick A. Hauck
    • H01M4/02H01M6/04H01M8/22H01M10/28
    • H01M8/225H01M6/04H01M2004/024
    • A replaceable electrode primary battery utilizing hollow zinc anodic electrodes and hollow nickel oxide cathodic electrodes immersed in a potassium hydroxide electrolyte solution. The electrodes are arranged in stacks formed by electrically conducting guides contacting the outer surfaces of the spherical electrodes, the respective guides forming the battery anode and cathode. Fresh electrodes are added to the top of the stack from a supply of electrodes, causing a spent electrode to be ejected from the bottom of the stack. The ejected electrode floats to the surface of the electrolyte solution and is collected in a holding compartment. The spent electrodes may be reused by electroplating the appropriate material on the outer surface of the spherical shell. The battery finds particular utility with electric vehicles where electrodes may be dispensed from conventional filling stations.
    • 使用浸渍在氢氧化钾电解质溶液中的中空锌阳极和中空氧化镍阴极电极的可替换电极一次电池。 电极被布置成由与球形电极的外表面接触的导电引导件形成的堆叠,各个引导件形成电池阳极和阴极。 新鲜电极从电极供应到堆叠的顶部,导致废电极从堆叠的底部排出。 喷射的电极漂浮在电解质溶液的表面,并被收集在保持室中。 废电极可以通过在球壳的外表面上电镀合适的材料来重新使用。 电池特别适用于电动车辆,其中电极可以从常规加油站分配。
    • 75. 发明授权
    • Electrochemical cell containing corrosion inhibitor
    • 电化学电池含腐蚀抑制剂
    • US3970476A
    • 1976-07-20
    • US590711
    • 1975-06-26
    • Pierre Cerfon
    • Pierre Cerfon
    • H01M4/62H01M6/04H01M17/00
    • H01M4/628H01M6/04
    • An electrochemical cell having a zinc negative electrode, a positive electrode, a saline electrolyte and a corrosion inhibitor added to the saline electrolyte to prevent corrosion of the zinc electrode by the electrolyte is disclosed. The inhibitor is ascorbic acid, which is added to the saline electrolyte preferably in proportions comprised between 700 and 900 mg/l. The mixture of the electrolyte and inhibitor is generally in paste form. The resultant inhibitor-containing electrolyte in practice does not corrode the zinc negative electrode of such cells during storage. Thus, prolonged storage of such cells, even in adverse tropical environments is possible.
    • 公开了一种具有锌电极,正电极,盐水电解质和腐蚀抑制剂的电化学电池,其被添加到盐水电解质中以防止电解质对锌电极的腐蚀。 抑制剂是抗坏血酸,优选以700-900mg / l的比例加入到盐水电解液中。 电解质和抑制剂的混合物通常为糊状。 所得到的含抑制剂的电解质实际上不会在储存期间腐蚀这种电池的锌负电极。 因此,即使在不利的热带环境中,这种细胞的长期储存是可能的。