热词
    • 80. 发明授权
    • Granulated kaolin compositions and processes for their production
    • 颗粒状高岭土组合物及其生产方法
    • US08388750B2
    • 2013-03-05
    • US12531597
    • 2008-03-20
    • Ernest GayJose MessiasSayre MenderRobert J. Pruett
    • Ernest GayJose MessiasSayre MenderRobert J. Pruett
    • C04B14/04C04B33/04
    • D21H17/68C01P2004/50C01P2004/60C01P2006/10C04B33/04C04B35/6263C04B35/62655C04B35/62695C04B35/63424C04B2235/5427C04B2235/5436C04B2235/5472C09C1/42Y10T428/2982
    • Disclosed herein are granulated kaolin compositions exhibiting at least one of improved material handling properties, low dusting during transit, easy make-down into mineral-water slurries, and requiring less energy to produce than spray dried kaolin products. The granulated kaolin compositions may, in one embodiment, be characterized by a moisture content ranging from about 12% to about 23% by weight relative to the total weight of the composition. In another embodiment, the granulated kaolin compositions may have an average granule size of greater than about 10 mesh. Also disclosed herein are granulated kaolin compositions having a moisture content ranging from about 12% to about 23% by weight relative to the total weight of the composition, wherein the composition is friable when subjected to a shear force. Further disclosed herein is a method for producing granulated kaolin compositions comprising mixing at least one kaolin slurry with at least one predispersed spray dried kaolin and agglomerating the resulting mixture. Still further disclosed herein is a system for producing granulated kaolin compositions comprising a first zone for mixing at least one kaolin slurry with at least one predispersed spray dried kaolin and a second zone for agglomerating the resulting mixture.
    • 本文公开了颗粒状高岭土组合物,其表现出改进的材料处理性能,运输过程中的低粉尘,容易地变成矿泉水浆料,并且比喷雾干燥的高岭土产品需要更少的能量产生中的至少一种。 在一个实施方案中,所述颗粒状高岭土组合物的特征在于相对于所述组合物的总重量为约12重量%至约23重量%的水分含量。 在另一个实施方案中,颗粒状高岭土组合物可以具有大于约10目的平均颗粒尺寸。 本文还公开了颗粒状高岭土组合物,其相对于组合物的总重量为约12重量%至约23重量%的水分含量,其中当经受剪切力时该组合物易碎。 本文进一步公开的是制备颗粒状高岭土组合物的方法,包括将至少一种高岭土浆料与至少一种预分散的喷雾干燥的高岭土混合并使所得混合物凝聚。 本文还进一步公开了一种用于生产颗粒状高岭土组合物的系统,其包含用于将至少一种高岭土浆料与至少一种预分散的喷雾干燥高岭土混合的第一区域和用于使所得混合物附聚的第二区域。