热词
    • 72. 发明申请
    • Interference pigments on the basis of silicon oxides
    • 基于氧化硅的干涉颜料
    • US20090169499A1
    • 2009-07-02
    • US12380364
    • 2009-02-26
    • Patrice BujardHolger Leybach
    • Patrice BujardHolger Leybach
    • C04B14/04C03C8/00A61Q5/10A61K8/25A61Q1/02
    • C09C1/0024C01P2004/54C09C2200/1037C09C2200/301C09D5/36Y10T428/2991Y10T428/2993
    • The present invention relates to pigments, the particles of which generally have a length of from 2 μm to 5 mm, a width of from 2 μm to 2 mm, and a thickness of from 20 nm to 2 μm, and a ratio of length to thickness of at least 2:1, wherein the particles contain a core of SiO2 or a silicon/silicon oxide obtained by heating SiOy flakes with 1.1≦y≦1.8 in an oxygen-free atmosphere at a temperature of at least 400° C., which core has a narrow distribution of particle sizes and two substantially parallel faces, the distance between which is the shortest axis of the core, and a material layer having a high index of refraction a metal oxide; a process for their production and their use in paints, ink-jet printing, for dyeing textiles, for pigmenting coatings (paints), printing inks, plastics, cosmetics, glazes for ceramics and glass.
    • 本发明涉及颜料,其颗粒通常具有2μm至5mm的长度,2μm至2mm的宽度和20nm至2μm的厚度,并且其长度与 至少2:1的厚度,其中所述颗粒含有通过在无氧气氛中在至少400℃的温度下加热1.1≤y≤1.8的SiO y薄片而获得的SiO 2核心或硅/氧化硅 ,该芯具有窄的粒度分布和两个基本上平行的面,其间的距离是芯的最短轴线,以及具有高折射率金属氧化物的材料层; 用于油漆,喷墨印刷,染色纺织品,着色涂料(油漆),印刷油墨,塑料,化妆品,陶瓷和玻璃的釉料的生产过程。
    • 73. 发明申请
    • Process of Using Microwave Deposition of Metal Oxide Onto an Organic Substrate
    • 将金属氧化物微波沉积到有机基板上的过程
    • US20080185099A1
    • 2008-08-07
    • US11792746
    • 2005-12-05
    • Patrice BujardRong Xiong
    • Patrice BujardRong Xiong
    • B32B38/10
    • C09C1/0018C01P2004/20C01P2004/54C01P2004/61C09C1/0024C09C1/0051C09C2200/1004C09C2220/106Y10T156/1158Y10T156/19
    • The present invention is directed to a process for the preparation of a plane-parallel structure (a platelet-shaped body, or flake), comprising at least one dielectric layer consisting of one or more oxides of a metal selected from groups 3 to 15 of the periodic table, which comprises the steps of: (a) applying a thin film of the dielectric material on a flexible belt, by passing the belt through an aqueous solution of a fluorine scavenger and one or more fluorine containing metal complexes which are the precursors of the desired metal oxide coating; and subjecting said solution to microwave radiation to deposit the metal oxide onto said flexible belt, wherein step (a) can optionally be repeated using different fluorine containing metal complexes to produce one or more metal oxide layers or a gradient of concentration of 2 different metal oxides across the thickness; (b) separating the resulting layer from the flexible belt as plane-parallel structures.
    • 本发明涉及一种制备平面平行结构(片状体或薄片)的方法,该方法包括至少一个由一种或多种金属氧化物构成的电介质层,所述金属氧化物选自 周期表,其包括以下步骤:(a)通过使带穿过氟清除剂的水溶液和作为前体的一种或多种含氟金属络合物,将电介质材料的薄膜施加在柔性带上 的所需金属氧化物涂层; 并将所述溶液经微波辐射将金属氧化物沉积到所述柔性带上,其中步骤(a)可任选地使用不同的含氟金属络合物重复以产生一种或多种金属氧化物层或浓度为2种不同金属氧化物的梯度 横跨厚度; (b)将所得层与柔性带分离成平面 - 平行结构。