    • Process for the preparation of polymerizable polyurethane elastomers
    • 制备可聚合聚氨酯弹性体的方法
    • US4334034A
    • 1982-06-08
    • US231836
    • 1981-02-05
    • August LehnerHeinrich HartmannGuenter HeilWerner LenzIngolf BuetheRudolf Bachmann
    • August LehnerHeinrich HartmannGuenter HeilWerner LenzIngolf BuetheRudolf Bachmann
    • C08G18/00C08G18/67C08G63/76C08G18/62
    • C08G18/6705C08G18/675
    • A process for the preparation of polymerizable, primarily linear thermoplastic polyurethane elastomers with acrylate side groups comprising reacting an organic polyisocyanate with a mixture of(a) an acrylate diol having a molecular weight of 146 to 3000,(b) an organic polyhydroxyl compound other than those of paragraph (a) having a molecular weight between 400 and 5000, and(c) a chain extender selected from the group consisting of diols, diamines, aminoalcohols, and triols, having molecular weights between 61 and 400, water, and mixtures thereofwherein the ratio of isocyanate to active hydrogen containing groups is from 0.8:1 to 1.2:1 and wherein 1.4 to 1.8 moles of organic polyisocyante, 0 to 15 moles of component (c) and 0.3 to 6 moles of component (a) are used per mole of component (b). The polymerizable polyurethane elastomers may be used for the manufacture of molded parts, laminates, adhesives, coatings, magnetic tapes, and other articles.
    • 一种制备具有丙烯酸酯侧基的可聚合的主要线性的热塑性聚氨酯弹性体的方法,包括使有机多异氰酸酯与(a)分子量为146至3000的丙烯酸酯二醇和(b)有机多羟基化合物的混合物 段落(a)分子量在400和5000之间的那些,和(c)分子量在61和400之间的选自二醇,二胺,氨基醇和三醇的增链剂,水及其混合物 其中异氰酸酯与含活性氢的基团的比例为0.8:1至1.2:1,并且其中使用1.4至1.8摩尔有机聚异氰酸酯,0至15摩尔的组分(c)和0.3至6摩尔的组分(a) 每摩尔组分(b)。 可聚合的聚氨酯弹性体可用于制造模制件,层压材料,粘合剂,涂料,磁带和其它制品。