    • Provided is a method for producing a platinum group-based alloy capable of producing a sound molten ingot of a platinum group-based alloy in a large amount. The method for producing a platinum group-based alloy includes a molten ingot production step of a continuous casting system using a plasma arc melting furnace configured to form a plasma arc column between an electrode torch which is arranged in an upper part of a vacuum chamber and a water cooled copper crucible which is arranged in a lower part of the chamber and has a cavity having a sectional area S1, the molten ingot production step including: inserting and melting an end part of a raw material bar including a platinum group-based alloy in the plasma arc column to cause the raw material bar to fall in drops on a base material in the water cooled copper crucible, to thereby form a molten pool; and solidifying a bottom part of the molten pool while maintaining a constant liquid level height of the molten pool by pulling down the base material, the molten ingot having a horizontal sectional area S (mm2) and a length L (mm) satisfying the following relationship: S1≧S>500, L>4√(S/π), an internal pressure of the chamber during melting being 0.8 atm or more, a pulling down speed of the base material being 10 mm/min or less.
    • 本发明提供能够大量生成铂族系合金的声熔体的铂族系合金的制造方法。 铂族系合金的制造方法包括使用等离子体电弧熔炼炉的连铸系统的熔融铸锭制造工序,该等离子体电弧熔融炉被配置为在设置在真空室的上部的电极炬之间形成等离子体电弧柱, 水冷铜坩埚,其布置在所述室的下部,并且具有截面积S1的空腔,所述熔池生产步骤包括:将包含铂族基合金的原料棒的端部插入和熔化 在等离子体电弧柱中使原料棒落在水冷铜坩埚中的基材上,从而形成熔池; 并且通过下拉基材来维持熔池的恒定的液面高度来固化熔池的底部,熔融铸锭的水平截面积S(mm2)和长度L(mm)满足以下关系 :S1≥S> 500,L>4√(S /π),熔融时的室内压为0.8atm以上,基材的拉下速度为10mm / min以下。