    • 51. 发明授权
    • Process and catalyst for producing polyolefins having low molecular weight
    • 用于生产低分子量聚烯烃的方法和催化剂
    • US06376418B1
    • 2002-04-23
    • US09559775
    • 2000-04-27
    • Edwar S. ShamshoumB. Raghava ReddyMargarito Lopez
    • Edwar S. ShamshoumB. Raghava ReddyMargarito Lopez
    • B01J3100
    • C08F10/00C08F4/61912C08F4/61927C08F110/02C08F110/06Y10S526/943C08F2500/02C08F2500/03
    • The invention provides a metallocene catalyst for use in preparing polyolefins having low molecular weight. The catalyst comprises a bridged metallocene in which one of the cyclopentadienyl rings is substituted in a substantially different manner from the other ring. The catalyst comprises a metallocene compound generally described by the formula R″(C5R4)(R′2C5C4R′4)MeQp wherein (C5R4) is a substituted cyclopentadienyl ring; (R′2C5C4R′4n) is an indenyl ring or substituted indenyl ring; each R and R′ is hydrogen or hydrocarbyl radical having from 1-20 carbon atoms, a halogen, an alkoxy, and alkoxy alkyl or an alkylamino radical, each R and R′ may be the same or different; (C5R4) has one R substituent in a distal position which is at least as bulky as a t-butyl radical; R″ is a structural bridge between the (C5R4) and (R′2C5C4R′4) rings to impart stereorigidity; Q is a hydrocarbyl radical, such as an alkyl, aryl, alkenyl, alkylaryl or arylalkyl radical having 1-20 carbon atoms or is a halogen; Me is a Group IIIB, IVB, VB, or VIB metal as positioned in the Periodic Table of Elements; and p is the valence of Me minus 2.
    • 本发明提供用于制备低分子量聚烯烃的茂金属催化剂。 该催化剂包括其中一个环戊二烯基环以与另一个环基本不同的方式被取代的桥连茂金属。 该催化剂包含一般由式R“(C5R4)(R'2C5C4R'4)MeQp描述的茂金属化合物,其中(C5R4)是取代的环戊二烯基环; (R'2C5C4R'4n)是茚基环或取代的茚基环; 每个R和R'是氢或具有1-20个碳原子的烃基,卤素,烷氧基和烷氧基烷基或烷基氨基,每个R和R'可以相同或不同; (C5R4)在远端位置具有至少与叔丁基一样庞大的一个R取代基; R“是(C5R4)和(R'2C5C4R'4)环之间的结构桥,以赋予立体刚度; Q是烃基,例如具有1-20个碳原子的烷基,芳基,烯基,烷基芳基或芳基烷基,或者是卤素; Me是位于元素周期表中的IIIB,IVB,VB或VIB族金属; 而p是Me的价数减去2。
    • 54. 发明授权
    • Compositions and systems for combatting lost circulation and methods
    • 打击流通和方法的组成和制度
    • US09518210B2
    • 2016-12-13
    • US13460266
    • 2012-04-30
    • Ryan G. EzellB. Raghava Reddy
    • Ryan G. EzellB. Raghava Reddy
    • C09K8/504C09K8/508C09K8/512
    • C09K8/5045C09K8/508C09K8/512
    • A method of servicing a wellbore in a subterranean formation comprising placing a first stream comprising a dilute solution of a metal acrylate into a lost circulation zone in the subterranean formation; placing a second stream comprising an activator into the lost circulation zone; and forming a lost circulation material upon contacting of the metal acrylate and the activator, wherein the lost circulation material forms in from about 0 to about 60 minutes. A method of servicing a wellbore in a subterranean formation comprising placing a composition comprising a dilute solution of a cross-linkable material and an encapsulated activator into a lost circulation zone in the subterranean formation; and allowing the composition to set.
    • 一种在地下地层中维护井眼的方法,包括将包含金属丙烯酸酯的稀溶液的第一物流放置在地下地层的失水循环区中; 将包含活化剂的第二物流放入所述丢失循环区中; 以及在金属丙烯酸酯和活化剂接触时形成漏失循环材料,其中所述失水循环材料形成约0至约60分钟。 一种在地下地层中维护井眼的方法,包括将包含可交联材料的稀溶液和包封的活化剂的组合物放置在地层中的失水循环区域中; 并允许组合物设定。
    • 55. 发明授权
    • Gellable treatment fluids having adjustable gel times and methods associated therewith
    • 可凝胶化处理液具有可调凝胶时间和与之相关的方法
    • US09175206B2
    • 2015-11-03
    • US13454827
    • 2012-04-24
    • B. Raghava ReddyLarry S. EoffFreddy Crespo
    • B. Raghava ReddyLarry S. EoffFreddy Crespo
    • C09K8/508C09K8/512
    • C09K8/882C09K8/5083C09K8/512C09K8/887
    • Gellable treatment fluids may have their gel times modified by using a polymer mixture therein that contains two or more polymers having disparate average molecular weights. Methods for treating a subterranean formation using such gellable treatment fluids can comprise providing a gellable treatment fluid comprising a polymer mixture and a crosslinking agent, introducing the gellable treatment fluid into a subterranean formation, and allowing the gellable treatment fluid to form a gel in the subterranean formation. The polymer mixture comprises a base polymer and an addend polymer, where the base polymer and the addend polymer each comprise an acrylamide monomer unit or a derivative thereof and have different average molecular weights, such that a molecular weight distribution of the polymer mixture contains at least two local maxima.
    • 可凝胶化处理液可以通过使用其中含有两种或更多种具有不同平均分子量的聚合物的聚合物混合物来改变凝胶时间。 使用这种可胶凝处理流体处理地下地层的方法可以包括提供包含聚合物混合物和交联剂的可凝胶化处理流体,将可凝胶化处理流体引入地层,并允许可凝胶化处理流体在地下形成凝胶 形成。 聚合物混合物包含基础聚合物和加成聚合物,其中基础聚合物和加成聚合物各自包含丙烯酰胺单体单元或其衍生物,并且具有不同的平均分子量,使得聚合物混合物的分子量分布至少包含 两个本地最大值。
    • 59. 发明授权
    • Wellbore cementing compositions and methods of making and using same
    • 井筒固井组合物及其制备和使用方法
    • US08720562B2
    • 2014-05-13
    • US12907209
    • 2010-10-19
    • B. Raghava ReddyRahul Chandrakant PatilSandip Pati
    • B. Raghava ReddyRahul Chandrakant PatilSandip Pati
    • E21B33/13
    • C09K8/467C04B24/38C04B24/383C04B28/02C09K8/487C04B20/023C04B20/04
    • A method of cementing a wellbore comprising preparing a wellbore cementing composition comprising a cementitious materials and a modified biopolymer additive wherein the modified biopolymer additive is the reaction product of a process comprising contacting a biopolymer and an organic carbonate to form a reaction mixture and subjecting the reaction mixture to a temperature of from about 100° F. to about 250° F. and placing the wellbore cementing fluid in the wellbore. A method of cementing a wellbore comprising contacting a modified biopolymer additive with a cementitious slurry to produce a wellbore cementing composition having an initial viscosity, v0; placing the wellbore cementing composition to a desired depth in a subterranean formation wherein the wellbore cementing composition has a transitional viscosity, vt, during placement in the subterranean formation and a final viscosity, vf, at the desired depth wherein vf≧vt>v0; and allowing the wellbore cementing composition to set.
    • 一种固井井的方法,包括制备包含水泥质材料和改性生物聚合物添加剂的井眼胶结组合物,其中改性生物聚合物添加剂是包括使生物聚合物和有机碳酸酯接触以形成反应混合物并使反应 混合物至约100°F至约250°F的温度,并将井眼固井液置于井筒中。 一种固井井的方法,包括使改性的生物聚合物添加剂与水泥浆料接触以产生具有初始粘度v0的井眼胶结组合物; 将井眼胶结剂组合物放置在地下地层中所需的深度,其中井眼胶结剂组合物在放置在地层中时具有过渡粘度vt,并且在期望深度处具有最终粘度vf,其中vf≥vt> v0; 并允许井筒固井组合物固化。
    • 60. 发明申请
    • LEWIS ACID AS GELATION RETARDER FOR CROSSLINKABLE POLYMER COMPOSITIONS
    • LEWIS ACID作为可交联聚合物组合物的凝胶阻滞剂
    • US20130056199A1
    • 2013-03-07
    • US13665151
    • 2012-10-31
    • B. Raghava ReddyLarry S. EoffJulio Estuardo VasquezEldon Dwyann Dalrymple
    • B. Raghava ReddyLarry S. EoffJulio Estuardo VasquezEldon Dwyann Dalrymple
    • C09K8/588E21B43/22
    • C09K8/512C09K8/5083C09K8/882C09K8/887
    • A treatment fluid for a well including: (a) a water-soluble polymer, wherein the water-soluble polymer comprises a polymer of at least one non-acidic ethylenically unsaturated polar monomer; (b) an organic crosslinker comprising amine groups, wherein the organic crosslinker is capable of crosslinking the water-soluble polymer; (c) a Lewis acid; and (d) water; wherein the treatment fluid is a crosslinkable polymer composition. According to an embodiment, a method for blocking the permeability of a portion of a subterranean formation penetrated by a wellbore is provided, the method including the steps of: (a) selecting the portion of the subterranean formation to be treated; (b) selecting estimated treatment conditions, wherein the estimated treatment conditions comprise temperature over a treatment time; (c) forming the treatment fluid; and (d) injecting the treatment fluid through the wellbore into the portion of the subterranean formation.
    • 一种用于井的处理流体,包括:(a)水溶性聚合物,其中所述水溶性聚合物包含至少一种非酸性烯属不饱和极性单体的聚合物; (b)包含胺基的有机交联剂,其中所述有机交联剂能够交联所述水溶性聚合物; (c)路易斯酸; 和(d)水; 其中所述处理流体是可交联聚合物组合物。 根据一个实施例,提供了一种用于阻挡由井眼穿透的地下地层的一部分渗透性的方法,所述方法包括以下步骤:(a)选择待处理的地层的部分; (b)选择估计的治疗条件,其中估计的治疗条件包括治疗时间以上的温度; (c)形成处理液; 和(d)将处理流体通过井眼注入到地层的部分中。