    • Polymers of vinyl oxazoline drying oil esters made by an improved process
    • 乙烯基恶唑啉干燥油酯的聚合物通过改进的方法制成
    • US4368309A
    • 1983-01-11
    • US328844
    • 1981-12-09
    • Joseph A. Vasta
    • Joseph A. Vasta
    • C07D263/14C08F242/00C08L1/10C08L1/14C09D3/74
    • C07D263/14C08F242/00
    • Polymers of vinyl oxazoline drying oil ester which esters are made by a process which reacts drying oil fatty acids with tris(hydroxy methyl) amino methane to form an intermediate which intermediate is further reacted at about 175.degree.-195.degree. C. with a formaldehyde/alcohol solution to form the vinyl oxazoline drying oil ester; the improvement used with this process is the use of at least 3 moles of formaldehyde to one mole of intermediate and about 1-5% by weight, based on the weight of the intermediate, of methanol and adding after the reaction with formaldehyde about 5-25% by weight, based on the weight of the ester solution, of an alcohol, a ketone or a mixture of an alcohol and a ketone; coating compositions of these polymers are also disclosed.
    • 乙烯基恶唑啉干燥油酯的聚合物,其通过使干油脂肪酸与三(羟甲基)氨基甲烷反应形成中间体的方法制备,所述中间体在约175-185℃下进一步与甲醛/ 醇溶液形成乙烯基恶唑啉干油酯; 使用该方法的改进是使用至少3摩尔甲醛至1摩尔中间体和约1-5重量%(基于中间体的甲醇重量),并在与甲醛反应后加入约5- 25重量%,基于酯溶液的重量,醇,酮或醇和酮的混合物; 还公开了这些聚合物的涂料组合物。
    • 44. 发明授权
    • Coating compositions of polymers of vinyl oxazoline drying oil esters
made by an improved process
    • 通过改进的方法制备乙烯基恶唑啉干燥油酯的聚合物的涂料组合物
    • US4368289A
    • 1983-01-11
    • US328845
    • 1981-12-09
    • Joseph A. Vasta
    • Joseph A. Vasta
    • C07D263/14C08F242/00C09D139/04C08L1/10C08L1/14C09D3/74
    • C08F242/00C07D263/14C09D139/04
    • A coating composition of polymers of a vinyl oxazoline drying oil ester which esters are made by a process which reacts drying oil fatty acids with tris (hydroxy methyl) amino methane to form an intermediate which is further reacted at about 175.degree.-190.degree. C. with a formaldehyde/alcohol solution to form the vinyl oxazoline drying oil ester; the improvement used with this process is the use of at least 3 moles of formaldehyde to one mole of intermediate and about 1-5% by weight, based on the weight of the intermediate, of methanol and adding after the reaction with formaldehyde about 5-25% by weight, based on the weight of the ester solution, of an alcohol, a ketone or a mixture of an alcohol and a ketone; the coating composition are aqueous and contain sufficient ammonia or amine to provide a pH of about 7.5-9.5.
    • 乙烯基恶唑啉干燥油酯的聚合物的涂料组合物,其酯通过使干性油脂肪酸与三(羟基甲基)氨基甲烷反应形成中间体的方法制备,所述中间体在约175-190℃进一步反应。 用甲醛/醇溶液形成乙烯基恶唑啉干油酯; 使用该方法的改进是使用至少3摩尔甲醛至1摩尔中间体和约1-5重量%(基于中间体的甲醇重量),并在与甲醛反应后加入约5- 25重量%,基于酯溶液的重量,醇,酮或醇和酮的混合物; 涂料组合物是含水的并且含有足够的氨或胺以提供约7.5-9.5的pH。