    • METHOD FOR MANUFACTURING WIRE, APPARATUS FOR MANUFACTURING WIRE, AND COPPER ALLOY WIRE
    • 制造线的方法,制造线的装置和铜合金线
    • US20090229715A1
    • 2009-09-17
    • US12398743
    • 2009-03-05
    • Isao TAKAHASHIKeisuke KITAZATO
    • Isao TAKAHASHIKeisuke KITAZATO
    • C21D9/62C22F1/08C22C9/00C22C9/06C22C9/02C22C9/04
    • H01B13/0016C21D1/40C21D9/62C22C9/00C22C9/06C22F1/00C22F1/08H01B1/026H01B13/0006
    • An apparatus for manufacturing wire comprising: a wire delivering equipment, a wire winding equipment, and an annealing while running equipment installed between the wire delivering equipment and the wire winding equipment, the age-precipitation copper alloy wire being passed in such manner that the wire turns around a plurality of times along a running route in the annealing while running equipment. The current applying equipment to raise a temperature of the age-precipitation copper alloy wire by generated Joule heat may be installed at upstream side of the annealing while running equipment. Another current applying equipment for solution treatment may be installed in tandem at upstream side of the annealing while running equipment. In place of the annealing while running equipment, a current applying equipment may be connected in tandem for age-treatment. By using those equipments, age-precipitation copper alloy wire having the diameter of from 0.03 mm to 3 mm may be obtained.
    • 一种用于制造线材的设备,包括:线材输送设备,绕线设备和安装在线材输送设备和线绕设备之间的设备的退火,该降水铜合金线材以这样的方式通过: 在运行设备的退火过程中沿着运行路线转动多次。 通过产生焦耳热提高年龄降低铜合金线的温度的当前施加设备可以安装在退火的上游侧,同时运行设备。 用于固溶处理的另一种当前施加设备可以在运行设备的退火的上游侧串联安装。 在运行设备时,代替退火,电流施加设备可以串联连接用于年龄处理。 通过使用这些设备,可以获得直径为0.03mm至3mm的年龄降低铜合金线。