    • 22. 发明授权
    • Corrosion resistant thermostat metal compositions
    • 耐腐蚀恒温金属组合物
    • US4366210A
    • 1982-12-28
    • US207011
    • 1980-11-14
    • Stanley M. Golemo, Jr.Anthony J. Izbicki
    • Stanley M. Golemo, Jr.Anthony J. Izbicki
    • B32B15/01B32B15/18
    • B32B15/011H01H2037/526Y10S428/925Y10T428/12507Y10T428/12958Y10T428/12979
    • Thermostat metals combining properties of relatively high flexivity and good corrosion resistance are prepared by metalurgically bonding a corrosion resistant high expansive alloy (1) to a less corrosion resistant low expansive alloy (2) and capping the low expansive alloy (2) with a corrosion resistant, moderately low expansive alloy (3) of similar hardness to that of the low expansive alloy (2).The preferred high expansive alloy (1) is comprised of about 18 wt. % Ni; 11 wt. % Cr; and balance Fe.The preferred low expansive alloy (2) is Invar (36 wt. % Ni; balance Fe).The preferred corrosion resistant low expansive alloy (3) is comprised of about 20 wt. % Ni; 26 wt. % Co; 7 wt. % Cr; balance Fe.The preferred volumetric ratios of the metals is about 50% of the high expansive alloy (1), 30 to 40% of the low expansive metal (2) and 10 to 20% of the corrosion resistant low expansive alloy.
    • 通过将耐腐蚀的高膨胀合金(1)与较低耐腐蚀的低膨胀合金(2)进行金相焊接并用低腐蚀性的低膨胀合金(2)封盖来制备具有相对高的柔性和良好的耐腐蚀性的恒温金属。 ,具有与低膨胀合金(2)相似硬度的中等低膨胀合金(3)。 优选的高膨胀合金(1)由约18wt。 %Ni; 11重量% %Cr; 并平衡Fe。 优选的低膨胀合金(2)是Invar(36重量%Ni;余量Fe)。 优选的耐腐蚀低膨胀合金(3)由约20wt。 %Ni; 26重量% %Co; 7重量% %Cr; 平衡铁 金属的优选体积比约为高膨胀合金(1)的50%,低膨胀金属(2)的30〜40%,耐腐蚀低膨胀合金的10〜20%。