热词
    • 22. 发明授权
    • Polymer granules having improved processability
    • 聚合物颗粒具有改善的加工性能
    • US5227455A
    • 1993-07-13
    • US939440
    • 1992-09-04
    • Peter IttemannGerhard Heinz
    • Peter IttemannGerhard Heinz
    • C08K5/07C08K5/3417C08K5/41C08L71/00C08L79/08
    • C08L79/08C08K5/07C08K5/3417C08K5/41C08L71/00
    • Premix for the production of mouldings, containingA) from 40-99.95% by weight of polymer granules A based on a polyaryl ether sulfone, polyaryl ether ketone, polyimide, polyamide imide or polyether imide, or a mixture thereof,B) up to 50% by weight of fillers B in fiber or particle form, or a mixture thereof,C) from 0.05-10% by weight of a compound C ether of the general formula X ##STR1## where A1 to A7 are identical or different and, independently of one another, are a radical of the formula --CO--, --O--, --S--, --SO.sub.2 --, --C(CH.sub.3).sub.2 --, a chemical bond, ##STR2## and k, l, m, n, p and q are each 0 or 1, or a C.sub.1 -C.sub.8 -alkyl, C.sub.1 -C.sub.8 -alkoxy or cyano derivative thereof which is substituted on the aromatic ring, or of the general formula Y ##STR3## where R is C.sub.1 -C.sub.8 -alkyl, C.sub.1 -C.sub.8 -alkoxy or cyano, A8 to A11 are as defined for A1 to A7, r, s and t are 0 or 1, and x is 2, 3 or 4, or a mixture thereof,is described.
    • 用于生产模制品的预混料,含有A)40-99.95重量%的基于聚芳基醚砜的聚合物颗粒A,聚芳基醚酮,聚酰亚胺,聚酰胺酰亚胺或聚醚酰亚胺,或其混合物,B)最多50 纤维或颗粒形式的填料B的重量%,或其混合物,C)0.05-10重量%的通式X(X)的化合物C醚,其中A1至A7为 相同或不同并且彼此独立地是式-CO - , - O - , - S - , - SO 2 - , - C(CH 3)2 - ,化学键, l,m,n,p和q各自为0或1,或其在芳环上被取代的C 1 -C 8 - 烷基,C 1 -C 8 - 烷氧基或氰基衍生物,或通式Y 其中R为C1-C8-烷基,C1-C8-烷氧基或氰基,A8至A11如A1至A7所定义,r,s和t分别为0或1,x为2,3或 4或其混合物。
    • 24. 发明授权
    • Preparation of polyaryleneetherketones
    • 聚乙二醇的制备
    • US5081215A
    • 1992-01-14
    • US393793
    • 1989-08-15
    • Juergen KochWolfgang StegmaierGerhard Heinz
    • Juergen KochWolfgang StegmaierGerhard Heinz
    • C08G65/40C08G61/12
    • C08G61/127
    • Polyaryleneetherketones are prepared by a quasicontinuous process, by Friedel-Crafts polycondensation of a reaction mixture containingA. a monomer system of(a)(1) an aromatic dicarboxylic acid chloride or phosgene and(2) a polynuclear aromatic having two exchangeable hydrogen atoms and/or(b) a polynuclear aromatic carboxylic acid chloride having one exchangeable hydrogen atom,B. a Lewis acid,C. if necessary, a Lewis base andD. an inert solvent.The reaction mixture is subjected to polycondensation in a first zone, with stirring, to a viscosity of not more than 2,000 mPa.s, then conveyed through a second, vertical, unstirred zone with plug flow by means of gas pressure, where the polycondensation is completed, and is finally discharged continuously.
    • 聚芳醚醚通过准连续法制备,通过Frieder-Crafts缩聚反应混合物,该反应混合物含有(a)(1)芳族二羧酰氯或光气的单体体系,和(2)具有两个可交换氢原子的多核芳烃和 /或(b)具有一个可交换氢原子的多核芳族羧酰氯,B.路易斯酸,C.如果需要,路易斯碱和D.惰性溶剂。 反应混合物在搅拌下在第一区域进行缩聚,粘度不大于2,000mPa.s,然后通过气体压力通过气流压力输送通过第二垂直的未搅拌区域,其中缩聚反应 完成,终于不停地出院。
    • 26. 发明授权
    • Heat-stable copolycondensate molding materials
    • 热稳定共缩聚成型材料
    • US4925910A
    • 1990-05-15
    • US36446
    • 1987-04-09
    • Gerhard Heinz
    • Gerhard Heinz
    • C08G65/40C08G75/00C08G75/20C08G75/23C08L71/00H05K1/03
    • C08G75/23C08G65/4012C08G75/20C08L71/00C08L2205/05H05K1/0333H05K1/0373
    • Copolycondensate molding materials are obtainable by polycondensation offrom 2 to 98 mol % of 2,2-di-(4'-hydroxyphenyl)-propane (A),from 2 to 98 mol % of 4,4'-dihydroxydiphenyl sulfone (B) andfrom 0 to 96 mol % of (C) ##STR1## where R.sup.1 and R.sup.2 are each H, C.sub.1 -C.sub.6 -alkyl or C.sub.1 -C.sub.6 -alkoxy, X is a chemical bond, --S--, --O--, --CO--, CR.sup.3 R.sup.4 (where R.sup.3 and R.sup.4 are different when n and p are each 0), or SO.sub.2 -- only when n or p is 0), R.sup.3 and R.sup.4 are each H, C.sub.1 -C.sub.6 -alkyl, C.sub.1 -C.sub.6 -alkoxy, aryl or halogen-substituted alkyl of 1 to 4 carbon atoms, m is 0 or 1, and n and p are each 0, 1, 2, 3, or 4,with from 1 to 100 mol % of (D) ##STR2## where R.sup.5 and R.sup.6 have the same meaning as R.sup.1 and R.sup.2, and v and w are each 0, 1, 2, 3 or 4, and from 0 to 99 mol % of (E) ##STR3## where R.sup.7 -R.sup.10 are each Cl or F or have the same meanings as R.sup.1 and R.sup.2, q is 0 or 1, r, s, t and n are each 0, 1, 2, 3 or 4, Z.sub.1 is --SO.sub.2 -- or --CO-- and Z.sub.2 is --O--, --S--, --SO.sub.2 --, --CO-- or a chemical bond,with the proviso that one or more of the components C and E are present and the molar ratio of B to the sum of A and C is not greater than 1.
    • 共缩聚成型材料可以通过2〜98摩尔%的2,2-二(4'-羟基苯基) - 丙烷(A),2〜98摩尔%的4,4'-二羟基二苯基砜(B)的缩聚得到, 和0至96摩尔%的(C)其中R 1和R 2各自为H,C 1 -C 6烷基或C 1 -C 6 - 烷氧基,X为化学键,-S - , - O - , - CO - ,CR 3 R 4(其中当n和p各自为0时,R 3和R 4不同)或者仅在n或p为0时为SO 2),R 3和R 4各自为H,C 1 -C 6烷基,C 1 -C 6 - 烷氧基, 1至4个碳原子的芳基或卤素取代的烷基,m为0或1,n和p各自为0,1,2,3或4,其中(D)为1至100摩尔% 其中R 5和R 6具有与R 1和R 2相同的含义,v和w各自为0,1,2,3或4,和0至99mol%的(E),其中R 7 -R 10各自为Cl 或F或具有与R 1和R 2相同的含义,q为0或1,r,s,t和n各自为0,1,2,3或4,Z 1为-SO 2 - 或-CO-,Z 2为 - O-,-S-,-SO 2 - , - CO-或化学键,条件是组分C和E中的一种或多种 并且B与A和C之和的摩尔比不大于1。
    • 28. 发明授权
    • Preparation of branched block copolymers
    • US4418180A
    • 1983-11-29
    • US296849
    • 1981-08-27
    • Gerhard HeinzBurghard SchmittIngo H. DornHermann GausepohlKarl GerberdingRudolf H. JungHans MittnachtJurgen PohrtPaul Witimer
    • Gerhard HeinzBurghard SchmittIngo H. DornHermann GausepohlKarl GerberdingRudolf H. JungHans MittnachtJurgen PohrtPaul Witimer
    • C08F297/04
    • C08F297/044
    • A process for the preparation of branched block copolymers of from 60 to 95% by weight of a monovinyl-aromatic monomer and from 40 to 5% by weight of a conjugated diene by polymerizing the monomers in an inert solvent in the presence of a monolithium-hydrocarbon as the initiator, wherein, in a first process stage (a), from 50 to 80, or where necessary at most 90, % by weight of the total amount of monovinyl-aromatic compound are polymerized to virtually complete conversion in the presence of a relatively small amount of the monolithium-hydrocarbon. This stage is carried out by starting with from 30 to 70% by weight of the vinyl-aromatic monomer and adding from 70 to 30% by weight in the feed, during the polymerization, in such a way that the polymerization temperature, which at the start of the polymerization is from 30.degree. to 40.degree. C., is kept at from 45.degree. to 70.degree. C., with use of reflux cooling. After all the monomer feed has been added, the reaction temperature is lowered to 30.degree.-40.degree. C. by evaporative cooling. In a second process stage (b), an additional amount of initiator is added to the reaction solution, after which from 1 to 30% by weight of the total amount of monovinyl-aromatic monomer can be added, the sum of the amounts of monovinyl-aromatic monomer added in the first and second process stages being at most 90% by weight of the total amount of monovinyl-aromatic monomer. The monovinyl-aromatic monomer added in the second process stage is polymerized to virtually complete conversion, employing the temperature profile described for stage (a). In process stage (c), the remainder of the monovinyl-aromatic monomer and all of the conjugated diene are added, at least predominantly in the form of a mixture, and polymerized so that the reaction temperature does not rise above 90.degree.-110.degree. C. Finally, after virtually complete conversion of the monomers, and preferably without prior cooling, a suitable liquid polyfunctional coupling agent is run in undiluted and the mixture of the linear block copolymers obtained, which still contain active terminal lithium-carbon bonds, is coupled, with stirring, to form branched block copolymers. The products prepared according to the invention are used for injection molding.