    • Control of silica scaling during acid leaching of lateritic ore
    • 控制红土矿石浸酸过程中二氧化硅结垢
    • US4399109A
    • 1983-08-16
    • US352537
    • 1982-02-26
    • Ralph K. IlerPaul B. QueneauMark W. Cooperrider
    • Ralph K. IlerPaul B. QueneauMark W. Cooperrider
    • C22B23/00C01G51/10C01G53/10C01G53/11C22B20060101C22B3/00C23F14/00
    • C22B23/043Y02P10/212
    • A method is provided for inhibiting the formation of silica scale on flash-pot surfaces during the multi-stage flashing of sulfuric acid pressure-leach slurry obtained following the continuous autoclave leaching of nickel lateritic ore at elevated temperature and pressure during which silica is dissolved, wherein the leach slurry is subjected to a high-temperature flash stage such that the slurry at the flash temperature is supersaturated in soluble silica, and wherein the slurry is thereafter subjected to at least one additional flash at an intermediate-temperature flash stage at which silica precipitates and tends to form a scale accompanied by a decrease in said supersaturation. The improvement resides in recycling a substantial portion of the slurry to the intermediate-temperature stage following flashing to the intermediate-temperature flash stage, the portion recycled being sufficient to effect a dilution in silica concentration of the slurry being flashed into the intermediate-temperature flash stage from the high-temperature stage, and continuing the recycling of flashed slurry to the intermediate-temperature flash stage, whereby silica scale formation at the intermediate-temperature flash stage is greatly inhibited. The pH of the recycling stream may be adjusted to further minimize silica deposition.
    • 提供了一种方法,用于在高温和高压下二氧化硅溶解的镍红土矿石的连续高压釜浸出之后获得的硫酸压力浸出浆液的多级闪蒸期间,抑制闪蒸罐表面上二氧化硅垢的形成, 其中浸出浆料经受高温闪蒸阶段,使得闪蒸温度下的浆料在可溶性二氧化硅中过饱和,然后在中间温度闪蒸阶段将浆料经历至少一次另外的闪蒸,其中二氧化硅 沉淀并趋于形成伴随着所述过饱和度降低的氧化皮。 改进之处在于将大部分浆料循环回到中间温度闪蒸阶段之后的中间温度阶段,再循环的部分足以使浆料的二氧化硅浓度稀释到闪蒸到中间温度闪蒸 从高温阶段开始,持续将闪蒸浆料回收到中温闪蒸阶段,从而大大抑制了中温闪蒸阶段的二氧化硅垢形成。 可以调节再循环流的pH以进一步最小化二氧化硅沉积。