    • 21. 发明授权
    • Magnetic film, manufacturing method thereof and thin film magnetic head
    • 磁膜,其制造方法和薄膜磁头
    • US07842408B2
    • 2010-11-30
    • US11820598
    • 2007-06-19
    • Kazue KudoGen OikawaYohji MaruyamaNoriyuki SaikiHiromi Shiina
    • Kazue KudoGen OikawaYohji MaruyamaNoriyuki SaikiHiromi Shiina
    • G11B5/33H04R31/00
    • G11B5/3116G11B5/1278G11B5/147G11B5/313Y10T29/49032Y10T428/115
    • Embodiments of the present invention provide a magnetic disk drive capable of allowing higher data transfer rates and higher recording densities. According to one embodiment, an upper magnetic core and lower magnetic core comprise a multi-layered magnetic film formed by alternately stacking a face-centered cubic (fcc) crystalline magnetic thin layer and a body-centered cubic (bcc) crystalline magnetic thin layer by plating. The plating bath is such that the temperature is about 30±1° C., pH is about 2.0−1.0 to 2.0+0.5, metal ion concentrations are about 5 to 25 (g/l) for Ni2+ and 5 to 15 (g/l) for Fe2+, saccharin sodium concentration is about 1.5±1.0 (g/l), sodium chloride concentration is about 25±5 (g/l), and boric acid concentration is about 25±5 (g/l). Since each layer's crystal structure is different from that of its adjacent lower layer, epitaxial growth is broken within each layer. Thus, since crystal grains are reduced in size, it is possible to lessen the decrease of the permeability μ at higher frequencies.
    • 本发明的实施例提供一种能够允许更高数据传输速率和更高记录密度的磁盘驱动器。 根据一个实施例,上磁芯和下磁芯包括通过交替地将面心立方(fcc)晶体磁性薄层和体心立方(bcc)结晶磁性薄层交替堆叠而形成的多层磁性膜, 电镀。 电镀浴温度为约30±1℃,pH为约2.0-1.0至2.0 + 0.5,Ni2 +和5至15(g / l)的金属离子浓度为约5至25(g / l) l)对于Fe2 +,糖精钠浓度约为1.5±1.0(g / l),氯化钠浓度约为25±5(g / l),硼酸浓度约为25±5(g / l)。 由于每个层的晶体结构与其相邻的下层的晶体结构不同,所以在每个层内外延生长被破坏。 因此,由于晶粒尺寸减小,因此可以降低较高频率下的磁导率μ的降低。
    • 22. 发明申请
    • Magnetic shield, manufacturing method thereof and thin film magnetic head employing the same
    • 磁屏蔽,其制造方法和使用该磁屏蔽的薄膜磁头
    • US20080002308A1
    • 2008-01-03
    • US11820554
    • 2007-06-19
    • Kazue KudoGen OikawaYohji MaruyamaNoriyuki SaikiHiromi Shiina
    • Kazue KudoGen OikawaYohji MaruyamaNoriyuki SaikiHiromi Shiina
    • G11B5/127
    • G11B5/3116G11B5/1278G11B5/3912G11B5/3967
    • Embodiments of the present invention provide a magnetic shield composed of size-controlled small crystal grains and provide a more after-write read noise free thin film magnetic head. According to one embodiment of the present invention, an upper magnetic shield uses a multi-layered magnetic film formed by alternately stacking a face-centered cubic (fcc) crystalline magnetic thin layer and a body-centered cubic (bcc) crystalline magnetic thin layer by plating. The plating bath is such that the temperature is 30±1° C., pH is about 2.0-1.0 to 2.0+0.5, metal ion concentrations are about 5 to 25 (g/l) for Ni2+ and 5 to 15 (g/l) for Fe2+, saccharin sodium concentration is about 1.5±1.0 (g/l), sodium chloride concentration is about 25±5 (g/l), and boric acid concentration is about 25±5 (g/l). Each layer's crystal structure is different from that of its upper and lower layers, which results in size-controlled small crystal grains since the epitaxial growth is broken. Since crystal grains are reduced in size, it is possible to suppress the after-write read noise and therefore attain a read head which allows recording at higher frequencies.
    • 本发明的实施例提供一种由尺寸控制的小晶粒组成的磁屏蔽,并提供更多的后写入无噪声薄膜磁头。 根据本发明的一个实施例,上磁屏蔽使用通过交替层叠面心立方(fcc)结晶磁性薄膜和体心立方(bcc)结晶磁性薄膜而形成的多层磁性膜, 电镀。 电镀浴温度为30±1℃,pH为约2.0-1.0〜2.0±0.5,Ni 2+ / SUP的金属离子浓度约为5〜25(g / l) > 5〜15(g / l),糖精钠浓度约为1.5±1.0(g / l),氯化钠浓度约为25±5(g / l) 硼酸浓度约为25±5(g / l)。 每层的晶体结构与其上层和下层的晶体结构不同,这导致尺寸控制的小晶粒,因为外延生长破裂。 由于晶粒尺寸减小,因此可以抑制写入后的读取噪声,从而获得允许以较高频率记录的读取头。