会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 11. 发明授权
    • Laminated roofing shingle
    • 层压屋顶瓦
    • US5666776A
    • 1997-09-16
    • US521235
    • 1995-08-30
    • Casimir Paul WeaverMatti KiikWilliam J. SchultzPatrick T. Stapleton
    • Casimir Paul WeaverMatti KiikWilliam J. SchultzPatrick T. Stapleton
    • E04D1/26E04D1/28
    • E04D1/26E04D2001/005
    • A shingle having a headlap section and a buttlap section with at least one portion of the buttlap section having a relatively uniform color and another portion of the buttlap section having a color gradient or gradation from light to dark. An illusion of depth or thickness is created on the portion of the buttlap section having the color gradient. The buttlap section defines in part the exposed weather surface of the associated shingle. The relatively uniform color portions may be formed on tabs or dragon teeth and the color gradient formed on a backer sheet disposed beneath the tabs. Openings between adjacent tabs expose the color gradient to view. A plurality of horizontal striations may be used to establish the desired color gradient from light to dark. The amount of tone and contrast may be selected to create the desired illusion of depth or thickness. The amount of contrast may be varied depending upon the color selected for each shingle. The number of horizontal striations and their width may also be varied to provide the desired color gradient.
    • 具有头部部分和对接部分的木瓦,其中所述对接部分的至少一部分具有相对均匀的颜色,并且所述对接部分的另一部分具有从浅到暗的颜色渐变或渐变。 在具有颜色渐变的对接部分的部分上产生深度或厚度的错觉。 对接部分部分地定义了相关屋顶的暴露的天气表面。 相对均匀的颜色部分可以形成在翼片或龙牙上,并且颜色梯度形成在设置在翼片下方的底板上。 相邻选项卡之间的开口会显示颜色渐变以查看。 可以使用多个水平条纹来建立从浅到暗的期望的颜色梯度。 可以选择色调和对比度以产生所需的深度或厚度的错觉。 对比度可以根据为每个木瓦选择的颜色而变化。 水平条纹的数量及其宽度也可以变化以提供期望的颜色梯度。
    • 14. 发明授权
    • Method of making wet process panels of composite wood material with
semi-matching contoured pressure plates
    • 用半匹配成型压板制作复合木材的湿法面板的方法
    • US4726881A
    • 1988-02-23
    • US730241
    • 1985-05-02
    • William J. Schultz
    • William J. Schultz
    • B27N3/20D21J1/00D21J1/04D21J1/18
    • D21J1/04B27N3/20D21J1/00B29K2311/14
    • Panels of composite wood material are formed in a wet process which includes depositing a layer of wet composite wood material in a mat on a press wire screen mesh and moving the screen mesh to carry the mat into a pressing position between a pair of spaced apart pressure plates having generally matching, contoured facing surfaces for shaping the outer face and a smoothly contoured back face of the panel. The back face of the panel is not flat and generally follows or matches the shape or contour of the outer face so that regions of high fiber stress and dense, brittle areas of high fiber compression are generally eliminated. The resulting finished panels having excellent machining qualities, more uniform surface coating absorption characteristics, more uniform thickness and less rapid moisture absorption properties, along with a lower tendency to check, crack or split.
    • 复合木材材料的面板是以湿法形成的,其中包括将湿复合木材材料层沉积在压丝网筛上的垫中,并移动筛网以将垫运送到一对隔开的压力 板具有大体上匹配的,轮廓的面对表面,用于成形外表面和平滑轮廓的面板。 面板的背面不平坦,通常与外表面的形状或轮廓相符或匹配,因此高纤维应力的区域和高纤维压缩的致密,脆性区域通常被消除。 所得到的成品面板具有优异的加工性能,更均匀的表面涂层吸收特性,更均匀的厚度和更少的快速吸湿性能,以及更低的检查,裂缝或分裂倾向。